Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Fluoroloy® A12 High Performance Seal Material

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Fluoroloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Fluoroloy® A12 High Performance Seal Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInformation provided by Saint-Gobain Performance Plastics.
Physical Properties Metric English Comments
Density 1.95 g/cc
0.0704 lb/in³
ASTM D792
Deformation 3.0 %

@Time 86400 sec
3.0 %

@Time 24.0 hour
13.8 MPa (2000 psi) load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength 13.8 MPa
2000 psi
ASTM D1708
Elongation at Break 180 %
180 %
ASTM D1708
Compressive Yield Strength 6.89 MPa

@Strain 1.00 %
999 psi

@Strain 1.00 %
ASTM D695
Coefficient of Friction 0.12
0.12
ASTM D3702
Thermal Properties Metric English Comments
Thermal Conductivity 0.247 W/m-K
1.71 BTU-in/hr-ft²-°F
ASTM D435
Maximum Service Temperature, Air 288 °C
550 °F
Minimum Service Temperature, Air -268 °C
-450 °F
Electrical Properties Metric English Comments
Volume Resistivity 8.20e+18 ohm-cm
8.20e+18 ohm-cm
ASTM D4496
Surface Resistance 6.30e+18 ohm
6.30e+18 ohm
ASTM D4496
Dielectric Constant 2.4

@Frequency 1.00e+6 Hz
2.4

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength >= 7.87 kV/mm
>= 200 kV/in
ASTM D149
Descriptive Properties Value Comments
Color Light Brown
Copyright © lookpolymers.com All Rights Reserved