Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4-200BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low maintenance mol.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® R-4 02 Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at elev.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 150 °C |
25.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2410EPR PEI 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 150 °C |
25.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 150 °C |
25.0 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 2410EPR PEI (Europe-Africa-Middle East) 40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. Resin is RoHS compliant. UL94 V0 listing. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 0.000 - 100 °C |
25.0 µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatib.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU2400 PEI 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP MF006S PP LNP* THERMOCOMP* MF006S is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 LNP* THERMOCOMP* PH0460A is a compound based on Nylon 6. Added feature of this material is: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66 NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 23.0 - 150 °C |
25.0 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem HU2400 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM HU2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem HU2410 PEI (Europe-Africa-Middle East) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications.
Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp MF006S PP (Asia Pacific) LNP* Thermocomp* MF006S is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia P.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SU PP LNP* THERMOCOMP* MF006SU is a compound based on Polypropylene containing 30% lass Fiber. Characteristics of this grade are: Heat Stabilized, Chemically Coupled, UV Stabilized. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP OF006A PPS - Branched LNP* THERMOCOMP* OF006A is a compound based on PPS - Branched resin containing 30% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX675 PPE+PA6 Noryl GTX* GTX675 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is mineral filled, conductive, and suitable for injection molding. The conductivity level is optimized to a.. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific) LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
25.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PH0460A PA 6 (Asia Pacific) LNP* Thermocomp* PH0460A is a compound based on Nylon 6 resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 45.0 µm/m-°C @Temperature 20.0 °C |
25.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4-200NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low mainten.. |