Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Engineered Polymers SEQUEL® 1718HF Engineered Polyolefin  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers SEQUEL® 1718HF Engineered Polyolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SEQUEL® 1718HF engineered polyolefin is designed for painted automotive exterior applications that require dimensional stability over a broad temperature range. This material exhibits excellent processability and low-temperature properties. Applications: Bumper side claddings, rockers, and other compartments that demand close dimensional tolerances Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ISO 1183
Linear Mold Shrinkage 0.0060 - 0.0090 cm/cm
0.0060 - 0.0090 in/in
as molded; ISO 294
0.0080 - 0.011 cm/cm
0.0080 - 0.011 in/in
after bake; ISO 294
Melt Flow 16 g/10 min
16 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.60 GPa
232 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 22.0 J
16.2 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
30.6 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228