Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Impact Test | 22.0 J | 16.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Asia Pacific) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP FARADEX MS003 PP (Europe-Africa-Middle East) LNP* Faradex* MS003 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 1718HF Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1718HF engineered polyolefin is designed for painted automotive exterior applications that require dimensional stability over a broad temperature range. This material exhibits.. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | multiaxial, 15 mph; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 2300 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2300 engineered polyolefin is designed for large mold-in-color automotive interior applications that require high stiffness and dimensional stability over a broad temperature r.. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | multiaxial, 15 mph; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 2325 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2325 engineered polyolefin is designed for mold-in-color automotive interior applications. This material exhibits excellent low-gloss surface appearance and processability. Ap.. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | multiaxial, 15 mph; ASTM D3763 |
Solvay Engineered Polymers SEQUEL® 2330 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2330 engineered polyolefin is designed for large mold-in-color automotive interior applications that require stiffness and good dimensional stability. This material exhibits e.. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | multiaxial, 2.2 m/s; ASTM D3763 |
Solvay Engineered Polymers DEXFLEX® 810HSF TPO
(discontinued **) Description: DEXFLEX® 810HSF is a thermoplastic olefinic elastomer (TPO) designed for large molded-in-color automotive exterior applications that require high flow characteristics for excellent pro.. |
|||
Impact Test | 22.0 J @Temperature -30.0 °C |
16.2 ft-lb @Temperature -22.0 °F |
Dynatup Impact, E at Max Load, Ductile; ASTM D3763 |
LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good sur.. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP LUBRICOMP VN001 Super Tough Nylon LNP* LUBRICOMP* VN001 is a compound based on Super Tough Nylon containing 2% MOS2. Added feature of th is grade is: Wear Resistant. |
|||
Impact Test | 22.0 J @Temperature 23.0 °C |
16.2 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66 LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI.. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing 50% Glass Fiber. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF00A PA 6 (Asia Pacific) LNP THERMOCOMP* PF00A is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 (Asia Pacific) LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | Multiaxial Impact; ISO 6603 |
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66 LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | During tempering at 650°C tempering temperature (2h + 2h) |
Assab Steels 8407 2M Hot Work Steel ASSAB 8407 is a chromium-molybdenum-vanadium-alloyed steel which is characterized by: Good resistance to abrasion at both low and high temperatures. High level of toughness and ductility Uniform .. |
|||
Impact Test | 22.0 J | 16.2 ft-lb | tempering temperature 200°C. Austenitizing temperature 1020°C. |
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Impact Test | 21.9 J @Temperature 22.8 °C |
16.2 ft-lb @Temperature 73.0 °F |
Rheometric, 5mph, 1/2" diameter tup, 3" diameter ring |
DuPont Bexloy® AXW502NC010 Modified Ionomer Resin
(discontinued **) A modified ionomer resin engineered for injection molded exterior automotive applications.Availability: North AmericaInformation provided by DuPont. |
|||
Impact Test | 22.0 J @Temperature -30.0 °C |
16.2 ft-lb @Temperature -22.0 °F |
MAII, E at Max Load, Ductile; ISO 6603-2 |
LyondellBasell Hifax™ CA186 Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, excellent paintability and paint durability, good processabi.. |