Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.60 GPa | 232 ksi | STN EN ISO 178 |
Plastcom SLOVALEN PC 51 C 40 LS/1M Polypropylene reinforced with mineral filler, UV stabilized Modified copolymer PP for injection molding with the content of 40% mineral filler, UV stabilized. Product meets glow wire test at 750°C. Delivered in full RAL color scale.Information Provided by P.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
Polyplastic Armlen® PP-2FR Polypropylene, Flame Retardant Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Shell Carilon® DP P1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
Total Finathene® 6006 HDPE, blow molding, pipe
(discontinued **) Finathene® 6006 is a high density polyethylene produced by the slurry loop low pressure polymerization process. Polymerization is conducted in the absence of any other comonomer. Finathene® 6006 h.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 1% secant at 0.05 in/min; ASTM D790A |
LyondellBasell Pro-fax 6331NW Polypropylene Homopolymer, Nucleated/Antistat Key Features: antistatic and nucleated polypropylene homopolymer resin, short cycle time, resists dust pickup, low odorApplications: lightweight containers, closures, hospital and institutional ware.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66 PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® A 30 S FN31 000000 Nylon 66, Flame Retardant PA 66, non-reinforced, injection molding, halogen-free flame retardant, improved flowabilityInformation provided by LANXESS. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Teknor Apex Sinpolene TPP2010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Automotive Applications; Housings Forms: Pellets Process.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 50 mm span, 5 mm/min, tangent; ASTM D790 |
A. Schulman PP 1248-01 Polypropylene High-Flow Homopolymer Polypropylene DescriptionPolypropylene PP 1248-01 is a high-flow homopolymer polypropylene nucleated and anti static designed for the high speed molding of thin-walled, multi-cavity parts. ApplicationTypical appl.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
Polyram PlusTek RB845 Nylon 6 for Injection Molding, Impact Modified Impact modified Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
Total PSI 8350 High Impact Polystyrene 8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ISO 178 |
Unipetrol PP MONSTEN® GH 005 Polypropylene Homopolymer Made for injection molding. LTHA stabilized. Homopolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM-D790 |
Polyram RamShine PS503 Polystyrene, Flame Retardant Flame retardant, high impact polystyrene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 2 mm/min, 4 mm; ISO 178 |
Chi Mei Kibiton® PB-5910 SBC High transparency, medium stiffness, toughness |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0437W30L Wollastonite Reinforced |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334C10L1 Calcium Reinforced |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Adell BD-10 Nylon 6, Ultra High Impact Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Ashley Polymers Ashlene® R3144 PC/PBT A thermoplastic alloy offering a high level of chemical resistance combined with high impact and excellent mechanical properties. Black.Data provided by the manufacturer |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436C40L1 Calcium Reinforced |
|||
Flexural Modulus | 1.60 GPa @Temperature 23.0 °C |
232 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PP TOUCH 34725 Polypropylene, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 236Q33 Nylon 6.6, Impact Modified SAXAMID 236Q33 is a impact-modified polyamide 6.6 injection-molding-grade with very good flow properties and outstanding toughness. Even at low temperatures this grade offers super-tough properties... |
|||
Flexural Modulus | 1.60 GPa @Temperature 23.0 °C |
232 ksi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH329B20 Polypropylene Homopolymer, 20% Glass Filled SAXALEN PPH329B20 is a 20% glass beads filled Polypropylene - Homopolymer intended for injection molding. Low shrinkage, low warpage gradeInformation provided by SAX Polymers |
|||
Flexural Modulus | 1.60 GPa | 232 ksi | ASTM D790 |
Braskem H 510 Bioriented Film Polypropylene Applications: Bioriented films for conversion; adhesive tapes; textile and food packing. Information provided by Braskem |