Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Melt Flow 5.4 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.4 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Yield 41.2 MPa
5970 psi
5 mm/min; ASTM D638
Flexural Strength 60.8 MPa
8820 psi
2.8 mm/min; ASTM D638
Flexural Modulus 2.16 GPa
313 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 1.96 J/cm

@Thickness 6.35 mm
3.67 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
B/50; ISO R306
Flammability, UL94 V-0

@Thickness 1.50 - 6.00 mm
V-0

@Thickness 0.0591 - 0.236 in
Copyright © lookpolymers.com All Rights Reserved