Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy FXTW30PE ASA Pearlescent GELOY ASA resin with copper-look for capstock extrusion. Outstanding weatherability.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Geloy XTWE280 ASA Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman Eastar 5445 PCTG Copolyester, Injection Molded
(discontinued **) Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t.. |
|||
Vicat Softening Point | >= 86.0 °C | >= 187 °F | At 1 kg; ASTM D1525 |
Iran Petrochemical (PCC) Tabriz 3630/1 High Impact Polystyrene
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Eastman E6838-889P Polyethylene
(discontinued **) Polyethylene E6838-889P is a formulation suggested for extrusion coating applications and has been used successfully in compounding. This product may be used for holding food during cooking.Applicat.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
ICO Polymers ICOTEXâ„¢ 520-5059 500 Micron LDPE Powder Description: ICOTEX 520-5059 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Information provided by ICO Polymers.A Sch.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50°C/h; 50N; 10x10x4mm; ISO 306/B50 |
SYNTHOS Krasten® 154 General Purpose Polystyrene Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – dishes, jars, Petri dishes, screw caps.Extrusion – blends with high impact polystyre.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | VST/A/50; ISO 306 |
Styrolution Polystyrol 486 M GR 2 PS Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® VH-0800 ABS, Unreinforced FR Flame-retardant ABS with excellent weather resistance that is used in the exterior of OA devices such as monitors, printers, fax machines, duplicators etc.Information provided by Samsung Cheil Indus.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
DuPont Nucrel® 0908HS Ethylene-Methacrylic Acid Copolymer Resin for Film and Extrusion Coating/Laminating 9.2 wt% Methacrylic Acid.Nucrel® 0908HS is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and blown/cast film operations desi.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSC 1540(EU) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50N (T° increase = 5°C/h); ASTM D1525B |
Total PSC 1540(AS) Crystal Polystyrene 1540 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle times when mixed with a high impact p.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman DuraStar DS1900HF Polymer, Natural Durastar DS1900HF polymer is a high flow grade of Durastar . Durastar DS1900HF flow lengths are increased 20-40% relative to Durastar DS1000 as shown by spiral flow testing. Other outstanding featur.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman DuraStar MN630 Polymer, Natural Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very .. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 1kg load; ASTM D1525 |
Eastman DuraStar MN631 Polymer, Natural Durastar Polymer MN631 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char.. |
|||
Vicat Softening Point | 86.1 °C | 187 °F | ASTM D1525 |
ExxonMobil LD 516.LN Molding, Extrusion and Compounding Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Vicat Softening Point | 86.1 °C | 187 °F | ASTM D1525 |
ExxonMobil LD 637.LI Molding, Extrusion and Compounding Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Vicat Softening Point | 86.1 °C | 187 °F | ASTM D1525 |
ExxonMobil LDPE LD 637.LI Low Density Polyethylene Resin Product Description: LD 637.LI is a high melt index LDPE homopolymer intended for injection molding or compounding applications requiring high flow. It is ideal for tamper-evident, tear-to-open clos.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50N; ISO 306 |
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | 50N; ISO 306 |
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 86.0 °C @Load 1.00 kg, Thickness 3.17 mm |
187 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers NPS80-1800B Injection Molding Grade, General Purpose Polystyrene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 86.1 °C | 187 °F | |
Dow Primacor® 4608 Ethylene Acrylic Acid (EAA) PRIMACOR® 4608 polymer containing 6.5% comonomer is an extrusion/ coextrusion coating and laminating resin. It is designed to provide excellent adhesion to metallic, paper and polyethylene substrat.. |
|||
Vicat Softening Point | 86.0 °C @Load 1.02 kg |
187 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem F 7018 LDPE Extrusion Coating Polyethylene LDPE F 7018 is a low-density polyethylene and has excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating; and injec.. |
|||
Vicat Softening Point | 86.1 °C | 187 °F | 50°C/hr; 50N; ASTM D1525 |
Arkema Group Solarkote® A200 Acrylic Superior UV protection and weatherability, ASTM Classification PMMA 0233V1Information provided by Arkema Group |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Huntsman Rexell® L2101 Injection Molding LLDPE
(discontinued **) Linear-low very low density copolymer, injection molding, FDA compliant.Features: High flow, flexible with excellent environmental stress crack (ESCR), and warpage resistance.Applications: Fitments,.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | ASTM D1525 |
Huntsman PE2049 Injection Molding Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good molding processability, produces parts that are flexible, and show excellent flatness in large projected areas.Applicat.. |
|||
Vicat Softening Point | 86.0 °C | 187 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East) GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |