Polymer Property : Vicat Softening Point = 86.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Cycolac® FR15 ABS
Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated.
Vicat Softening Point 86.0 °C
187 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Geloy XTWE280 ASA
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 86.0 °C
187 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 86.0 °C
187 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 86.0 °C
187 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Geloy XTWE280 ASA (Asia Pacific)
Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Eastman 1390P Polyethylene  (discontinued **)
Low-density polyethylene 1390P is used primarily in extrusion-coating applications that require fast line speeds and relatively low coating weights. When compared with other low-density polyethylen..
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
DuPont Nucrel® 30707HS Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating  (discontinued **)
7 wt% Acrylic Acid.Nucrel® 30707HS is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio..
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Huntsman PE5080 Extrusion Coating Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Excellent draw down, low neck-in, and excellent adhesion.Applications: Extrusion: coating grade and thin coatings.FDA Notes: Conforms to FDA regulation 21 CFR..
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
NOVA Chemicals Novapol® LM-4021-L LDPE Injection Molding Resin
Features: Medium flow LDPE with a good balance of toughness, softness, dimensional stability and processability Applications: Injection molding of caps, closures and other specialty productsInformat..
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
ICO Polymers ICOFLOâ„¢ 510-5061 1200 Micron LDPE Powder
Description: ICOFLO 510-5061 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Vicat Softening Point 86.0 °C
187 °F
resin; ASTM D1525
Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin
LDC801YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC801YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2..
Vicat Softening Point 86.0 °C
187 °F
50°C/h; 50N; 10x10x4mm; ISO 306/B50
SYNTHOS Krasten® 154 General Purpose Polystyrene
Improved heat resistance, very good rheological properties.Examples of Application:Injection moulding – dishes, jars, Petri dishes, screw caps.Extrusion – blends with high impact polystyre..
Vicat Softening Point 86.0 °C
187 °F
VST/A/50; ISO 306
Styrolution Polystyrol 486 M GR 2 PS
Description: Polystyrol 486 M is a normal flowing, high-impact grade that is especially suitable for blends with a high proportion of general-purpose Polystyrol (preferably Polystyrol 165 H or Polys..
Vicat Softening Point 86.0 °C
187 °F
B/50; ISO R306
Samsung Cheil Industries Starex® TX-0530T TRABS, Unreinforced
Information provided by Samsung Cheil Industries.
Vicat Softening Point 86.0 °C
187 °F
Rate "B" Loading 1 (120 degC/h 10N); ASTM Test
Styrolution Styrolux 684D SBC
Styrolux 684D is a thermoplastic styrene-butadiene block copolymer which is suitable for injection molding, extrusion, and thermoforming. It offers an outstanding combination of crystal clarity and..
Vicat Softening Point 86.0 °C
187 °F
Phr = 0
Shandong Rike Chemical HELIâ„¢ HL-2005 Weather-resistance Acrylic Impact Modifier (AIM)
Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c..
Vicat Softening Point 86.0 °C
187 °F
A50; DIN 53460
Lubrizol ESTANE® T5417 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 86.0 °C
187 °F
1kg load; ASTM D1525
Eastman DuraStar MN630 Polymer, Natural
Durastar Polymer MN630 has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN630 has very ..
Vicat Softening Point 86.0 °C
187 °F
1kg load; ASTM D1525
Eastman Eastar AN011 Copolyester
Eastar AN011 copolyester is a high flow product. Eastar AN011 flow lengths are increased 20-40% relative to Eastar AN001 as shown by spiral flow testing. Other outstanding features of Eastar are eas..
Vicat Softening Point 86.0 °C
187 °F
50N; ISO 306
Denka TE-30 Transparent Resin Polymer (MABS resin) ABS
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Vicat Softening Point 86.0 °C
187 °F
50N; ISO 306
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Vicat Softening Point 86.0 °C
187 °F
50N; ISO 306
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Vicat Softening Point 86.0 °C

@Load 1.00 kg,
Thickness 3.17 mm
187 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
Diamond Polymers GPPS BEADS Injection Molding Grade, General Purpose Polystyrene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP)
AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi..
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP)
AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In..
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
Dow Engage® 8480 Polyolefin Elastomer
Description: Engage® 8480 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in footwear applications and profile extrusion of tubing and hoses. It has good clari..
Vicat Softening Point 86.0 °C

@Load 1.02 kg
187 °F

@Load 2.25 lb
ASTM-D1525
Braskem F 7018 LDPE Extrusion Coating Polyethylene
LDPE F 7018 is a low-density polyethylene and has excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating; and injec..
Vicat Softening Point 86.0 °C

@Load 1.02 kg
187 °F

@Load 2.25 lb
ASTM-D1525
Braskem F7018 LDPE Injection Molding Polyethylene
F7018 is a low-density polyethylene with excellent processability and sealability at low temperatures. It does not contain additives. Its applications include: extrusion coating, injection molding ..
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525
DuPont Bynel® 41E558 Anhydride-Modified LLDPE Adhesive Resin  (discontinued **)
Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi..