Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HF380XC ABS, High Flow, High Surface Gloss Feature: Injection Molding, High Flow, High Surface GlossApplication: High melt flow index is suitable for injection molding of large and complicated part. High thermal stabilities enables to expres.. |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN133G33HIBL G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID HI1102B(W) PA66, High Impact Feature: Injection Molding,PA66, High ImpactApplication: Automotive (Covers)CAS No. 32131-17-2 and 9010-79-1Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN170SA General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | >= 1.96 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 3.67 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SC2302 PC+GF30%, High Impact Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.96 J/cm @Temperature 23.0 °C |
3.67 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUTENE-H PE0235 HDPE Description: LUTENE-H PE0235 is a materials with high toughness and rigidity suitable for cable protection It has very high resistance to stress cracking and long-term internal pressure creep proper.. |
|||
Izod Impact, Notched | >= 1.96 J/cm @Temperature 23.0 °C |
>= 3.67 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC PH162 HDPE Features: Characteristics : Good balance of toughness & stiffness stressAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 200-230°C (392-446°C) f.. |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | ASTM D256 |
Lotte Chemical Titan TITANZEX® HM5000 High density polyethylene HM5000 is a high density polyethylene for extrusion monofilament. HM5000 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3... |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN173MC M/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | ASTM D256 |
Global S-5000 High Density Polyethylene Description-good for monofilament Applications-ropes, fishing net, agricultural net and sports netInformation provided by Global Polymers Corporation. |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SE1V PPE+HIPS (Asia Pacific) PPE/HIPS, unfilled, FR-V1, 90 oC |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | |
Shinil Chemical SHINNANO PP Polymer Nanocomposite Door Trim SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® HF-0660I ABS, Unreinforced Material with high flowability and high stiffness that can be used for vacuum cleaner, telephone, TV, VCR, calculator, radio and air-conditionerInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® HF-0660IW ABS, Unreinforced WNP high flow ABS materialInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9120 ASA, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9370 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® CM-0140UV ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0860EX ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WR-9370 ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® WX-9300UV ASA, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® DMF3000S Polycarbonate, Anti-yellowing PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.DMF3000S is an anti-yellowing grade.Information provided by Samyang. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.35 mm |
3.67 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VE-0860EX ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N1052P PPE+HIPS (Asia Pacific) PPE+PS 105deg.C FR V-2 |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 3.17 mm |
3.67 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Izod Impact, Notched | 1.96 J/cm @Temperature 23.0 °C |
3.67 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Denka MALECCA K-200 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | ASTM D256 |
E-Polymers TEKALOY® S630XB Heat Resistance, Weatherability PC/PBT Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | ASTM D256 |
E-Polymers TEKAPPO® JF1 Un-Reinforced Flame Retardant M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
Izod Impact, Notched | 1.96 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.67 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
Asahi Kasei Xyron® X0700 Modified Polyphenylene Ether AutomotiveInformation provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.96 J/cm | 3.67 ft-lb/in | Method A; ASTM D256 |
Proto3000 PC-ABS Fused Deposition Modeling Polymer Description: PC-ABS (polycarbonate-ABS) is one of the most widely used industrial thermoplastics. PC-ABS offers the most desirable properties of both materials - the superior strength and heat resis.. |