Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® 48991A015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermabond® G2pr - electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberLiner: PolyethyleneProduct Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Light blue colored, high viscosity gum on fiberglass with polyethylene release liners.This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns
1.50 mil
Substrate; Arlon SQA-TMS-003
38.1 microns
1.50 mil
Liner
76.2 microns
3.00 mil
Liner
152 microns
6.00 mil
Side 1; Arlon SQA-TMS-003
152 microns
6.00 mil
Side 2; Arlon SQA-TMS-003
381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 5.86 MPa
850 psi
Silicone Property; ASTM D412
Elongation at Break 400 %
400 %
Silicone Property; ASTM D412
Modulus of Elasticity 0.00603 GPa
0.875 ksi
Silicone Property; Arlon SQA-TMS-008
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Shear Modulus 0.000276 GPa
0.0400 ksi
ASTM D1002
Shear Strength 5.86 MPa
850 psi
Lap; ASTM 1002
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C
100 µin/in-°F
Silicone Property; ASTM E 831
CTE, linear, Parallel to Flow 40.0 µm/m-°C
22.2 µin/in-°F
ASTM E 831
CTE, linear, Transverse to Flow 40.0 µm/m-°C
22.2 µin/in-°F
ASTM E 831
Specific Heat Capacity 0.960 J/g-°C
0.229 BTU/lb-°F
Product Property; E1461-01
1.14 J/g-°C
0.272 BTU/lb-°F
Silicone Property; E1461-01
Thermal Conductivity 0.300 W/m-K
2.08 BTU-in/hr-ft²-°F
Product Property; ASTM E 1530
0.400 W/m-K
2.78 BTU-in/hr-ft²-°F
Silicone Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg <= -100 °C
<= -148 °F
Silicone Property; ASTM D3418
Electrical Properties Metric English Comments
Dielectric Constant 3.2

@Frequency 1.00e+6 Hz
3.2

@Frequency 1.00e+6 Hz
Product Property; IPC TM 650 - 2.5.5.3
3.4

@Frequency 1.00e+6 Hz
3.4

@Frequency 1.00e+6 Hz
Silicon Property; IPC TM 650 - 2.5.5.3
Dielectric Strength 44.9 kV/mm
1140 kV/in
ASTM D149
Dissipation Factor 0.0040

@Frequency 1.00e+6 Hz
0.0040

@Frequency 1.00e+6 Hz
Product Property; IPC TM 650 - 2.5.5.3
0.0050

@Frequency 1.00e+6 Hz
0.0050

@Frequency 1.00e+6 Hz
Silicon Property; IPC TM 650 - 2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.0689 - 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 10.0 - 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 4.44 - 10.0 °C
6.00 Month

@Temperature 40.0 - 50.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Light Blue
Total Product Weight (g/m2) 439
Arlon SQA-TMS-025