SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets and FilmHoses and TubingShoe ComponentsFire HosesInformation provided by SK Chemicals.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Hardness, Shore D 44
44
ASTM D2240
Tensile Strength, Ultimate 53.9 MPa
7820 psi
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
100% Modulus 0.0103 GPa
1.50 ksi
ASTM D412
300% Modulus 0.0200 GPa
2.90 ksi
ASTM D412
Resilience 40
40
Vertical Rebound; ASTM D2632
Tear Strength 118 kN/m
672 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 40
40
H18 wheel, 1000g load; ASTM D1044
Thermal Properties Metric English Comments
Vicat Softening Point 110 °C
230 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 195 °C
383 °F
Transition Temperature
195 °C
383 °F
Metering Temperature
Middle Barrel Temperature 190 °C
374 °F
Nozzle Temperature 200 °C
392 °F
Zone 1 180 °C
356 °F
Zone 2 185 °C
365 °F
Zone 3 190 °C
374 °F
Zone 4 195 °C
383 °F
Adapter Temperature 195 °C
383 °F
Die Temperature 195 °C
383 °F
Tip
200 °C
392 °F
Body
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Users viewing this material also viewed the following: