Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.9 - 72.0 MPa
7820 - 10400 psi
Average value: 65.2 MPa Grade Count:19
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Ultimate 53.9 MPa
7820 psi
DIN 53455; ASTM D638
Kolon KOPA® KN333HI4 High Impact Nylon 66
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin..
Tensile Strength, Ultimate 53.9 MPa
7820 psi
DIN 53455; ASTM D638
Kolon KOPA® KN173HI3R High Impact Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Tensile Strength, Ultimate 53.9 MPa
7820 psi
ASTM D638
SK Chemicals SKYPEL M572CR Special Grade Copper Resistance
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Tensile Strength, Ultimate 53.9 MPa
7820 psi
ASTM D412
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 53.9 MPa
7820 psi
ASTM D412
SK Chemicals SKYTHANE® 590A X series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Ultimate 53.9 MPa
7820 psi
ASTM D412
Lubrizol Estane® S195A Thermoplastic Polyurethane
Type: Estane® S195A is a Shore 95A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, ..
Tensile Strength, Ultimate 53.9 MPa
7820 psi
ASTM D1708
Daelim H&L Plavis-G40 DF 40% Graphite Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-G-40: Graphite 40 wt% filled, Self lubricating grade with low thermal expansion.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is..
Tensile Strength, Ultimate 53.9 MPa
7820 psi
DIN 53455; ASTM D638
Kolon SPELLOY® KB133HF PC + PBT Alloy Resin  (discontinued **)
SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional..