Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D412 |
S&E Specialty Polymers G-4785E PVC Application: Flexible, PVC material designed for general-purpose extrusion applications.Information provided by S&E Specialty Polymers |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D412 |
Northstar Polymers MSB-A95A High Performance Polyurethane Cast Elastomer System This is a Ester/MDI base high-performance polyurethane casting system. This systems is recommended to applications in which the part requires high tensile strength, cut/tear resistance, dry-abrasio.. |
|||
100% Modulus | 0.0103 GPa | 1.49 ksi | |
Dow Pellethane® 2102-90AE Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AE elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with good damping capacity and good hydrolytic sta.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.0103 GPa | 1.49 ksi | |
LG Chemical LGflex GL100 Plasticizer Features: Excellent Heat Loss and Non-endocrine disrupter Application: PVC Power Cable, SheetsInformation provided by LG Chemical |
|||
100% Modulus | 0.0103 GPa | 1.49 ksi | |
Taiwan PU Corporation TPU-E95 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.0103 GPa | 1.49 ksi | |
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D412 |
SK Chemicals SKYTHANE® S392A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D412 |
SK Chemicals SKYTHANE® X590A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D412 |
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy Elastomeric Stat-Rite® Polymer alloy X-5065 blend is a patented inherently dissipative polymer (IDP) with thermoplastic polyurethanes (TPU). This produces soft, flexible polymer alloys with an in.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D412 |
Lubrizol Estane® ALR PC55D Thermoplastic Polyurethane Type: Estane® ALR PC60D is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
100% Modulus | 0.0103 GPa | 1.49 ksi | |
Elastomer Engineering E95C Polyurethane A high-performance, moderate cost formulation. A polyester/ether that combines many of the best properties of both polyester-based and polyether-based elastomers. Typical uses: Wheels, rolls, pist.. |
|||
100% Modulus | 0.0103 GPa | 1.49 ksi | JIS-K-6723 |
Denka VINYKON W7100N PVC, W grade for non-migratory sheath and special items A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D638 |
Colorite Polymers 8083 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | |
Colorite Polymers 8311 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | |
Colorite Polymers 8312 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D638 |
Colorite Polymers 8533 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D638 |
Colorite Polymers 8588 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | |
Colorite Polymers Self Frosting™ 8311SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D-638 |
Axiall 8833 Moldings & Extrusions Flexible PVC A clear, flexible PVC compound best suited for 80C automotive tubing applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D-638 |
Axiall 02541 Plenum Flexible PVC Non-lead stabilized CAT 3 jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D-638 |
Axiall 1131-57D Wire & Cable Flexible PVC Non-lead stabilized 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D-638 |
Axiall 22830 Coax & Telecom/Moldings & Extrusions Flexible PVC Non-lead stabilized, 75C rated jacketing compound suitable for CATV, CM, CL2 type applications. UL recognized for 94 V-0 in all colors at 1.5 mm. QMFZ2 recognized component.Information provided by.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D-638 |
Axiall 8870 Moldings & Extrusions Flexible PVC Economical general purpose extrusion and molding compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.0103 GPa | 1.50 ksi | ASTM D-638 |
Axiall 38831 Coax & Telecom Flexible PVC Category 5(+), flexible CMR jacket at 28-30 mils over HDPE inners.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.0103 GPa | 1.49 ksi | ASTM D412 |
Dow PELLETHANE® 2104-45D Polyurethane Elastomer (Ether-Ether Hybrid)
(discontinued **) Description: PELLETHANE® 2104-45D ether-ether hybrid polyurethane elastomer has excellent low temperature properties, fast cycle time, and good resistance to fuel and oils. Applications include: C.. |