Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Valox®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.13 %
0.13 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.36 %

@Temperature 23.0 °C
0.36 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0032 - 0.0040 cm/cm
0.0032 - 0.0040 in/in
on tensile bar; SABIC Method
Melt Flow 38 g/10 min

@Load 5.00 kg,
Temperature 265 °C
38 g/10 min

@Load 11.0 lb,
Temperature 509 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 95.0 MPa
13800 psi
ASTM D 638
105 MPa
15200 psi
5 mm/min; ISO 527
Tensile Strength, Yield 95.0 MPa
13800 psi
ASTM D 638
105 MPa
15200 psi
5 mm/min; ISO 527
Elongation at Break 1.8 %
1.8 %
ASTM D 638
2.0 %
2.0 %
5 mm/min; ISO 527
Elongation at Yield 1.8 %
1.8 %
ASTM D 638
2.0 %
2.0 %
5 mm/min; ISO 527
Tensile Modulus 6.25 GPa
906 ksi
5 mm/min; ASTM D 638
6.40 GPa
928 ksi
1 mm/min; ISO 527
Flexural Yield Strength 145 MPa
21000 psi
2 mm/min; ISO 178
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
Izod Impact, Notched 0.500 J/cm

@Temperature 23.0 °C
0.937 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
0.500 J/cm

@Temperature -30.0 °C
0.937 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
6.00 kJ/m²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 19.0 kJ/m²

@Temperature 23.0 °C
9.04 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
19.0 kJ/m²

@Temperature -30.0 °C
9.04 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact, Notched 0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 31.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
17.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
52.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Vicat Softening Point 230 °C
446 °F
Rate B/50; ISO 306
230 °C
446 °F
Rate B/120; ISO 306
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASS
IEC 60695-10-2
Copyright © lookpolymers.com All Rights Reserved