Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature -30.0 - 100 °C
52.2 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP
SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met..
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
52.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66
LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant.
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
52.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON PE002Z PA 6
LNP* STAT-KON* PE002Z is a compound based on Nylon 6 resin containing 10% Carbon Fiber. Added features of this grade include: Extrusion Grade.
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
52.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Thermocomp PK0049 PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PK0049 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include; Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Mid..
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
52.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON REF42I PA 66
LNP* STAT-KON* REF42I is a compound based on Nylon 6/6 containing Proprietary Fillers. Added feature of this grade is: Electrically Conductive.
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
52.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 2FL24 ETFE
LNP* THERMOCOMP* 2FL24 is a compound based on ETFE resin containing 20% Glass Fiber, 10% PTFE. Added feature of this grade is Wear Resistant.
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
52.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp 2FL24 FP-E (EFTE)
LNP* 2FL24 is a Fluoropolymer, ETFE grade containing Glass Fibers and PTFE.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
52.2 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
Styron EMERGEâ„¢ 5302 Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ ABS 5302 is a black, 20% glass-filled ABS which is suitable for use in a wide variety of internal structural component applications in the information technology market. Applications: ..
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
Eastman Eastar GN007 PETG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
52.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam PK0049 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded
Starflam PK0049 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
52.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-1/2
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
52.2 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East)
Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu..
CTE, linear, Transverse to Flow 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
ISO 11359
LG Chemical HG-174 ABS, High Gloss, Super High Flow
Information Provided by LG Chem