Unitika elitel UE3370 Polyester, Flake

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer Unitika
Trade Name elitel
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unitika elitel UE3370 Polyester, Flake.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low molecular weight type, High OH type, Low softening pointUNITIKA elitel resins are thermoplastic saturated copolymeric polyester resins. Elitel resins are expanding their applications from products such as adhesives, paints, ink binders, and modifying agents to the products in new-generation high-tech fields.Characteristics:elitel products have superior adhesiveness and coatability. They exhibit excellent adhesiveness and coatability to films and molded products of plastic materials such as polyester, polyvinylchloride, polycarbonate, and cellulose acetate; steel materials such as steel plates; metal materials such as copper, and aluminum; woven or nonwoven fabrics from polyester and other fibers; papers, woods, and others.elitel products may be hardened by combined use of a hardening agent.Blending of an elitel resin with another elitel resin or a different resin provides alloys with more diversified resin properties. Additionally, elitel products are effective as a modifying resin for providing other resins with flexibility, coatability, toughness, and others. elitel resins form films excellent in flexibility, electrical properties, weather resistance, as well in appearance and transparency: elitel resins retain consistent quality with smaller change in quality over time They are also excellent hygienically.Information provided by Unitika Ltd.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
JIS K-6911
Moisture Absorption at Equilibrium 0.30 %
0.30 %
60%RH
Molecular Weight 7000 g/mol
7000 g/mol
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 53.0 °C
127 °F
Chemical Properties Metric English Comments
Acid Value 3.0
3.0
[mgKOH/g}
Descriptive Properties Value Comments
Appearance Pale yellow
Hydroxyl Value 18 mgKOH/g