Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Modulus = 6.25 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 6.25 GPa
906 ksi
50 mm/min; ASTM D638
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK
Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers
Tensile Modulus 6.25 GPa
906 ksi
50 mm/min; ASTM D638
Ovation Polymers Nemcon™ H PK DP110/X5 Polyetheretherketone
Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All sa..
Tensile Modulus 6.25 GPa
906 ksi
Radici Radilon® S CP400 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Tensile Modulus 6.25 GPa
906 ksi
Radici Radilon® S RCP3010LK (cond.) Nylon 6
PA6 30% Glass Fiber and mineral filler reinforced injection molding grade. Good stiffness and good dimensional stability. Heat stabilized, good surface finish.Information provided by Radici group.
Tensile Modulus 6.25 GPa
906 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP PH0240A PA 6
LNP* THERMOCOMP* PH0240A is a compound based on Nylon 6 resin. Added features of this grade include: High Impact, High Specific Gravity.
Tensile Modulus 6.25 GPa
906 ksi
Storage
Epoxy Technology EPO-TEK® H31D Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H31D is a single component, electrically conductive silver epoxy designed for die-bonding of semiconductors, including IC’s, resistors, capacitors, transistors, and d..
Tensile Modulus 6.25 GPa
906 ksi
ISO 527
Eurotec® Tecolen® HP10 GR30 NL HS PPCP, 30% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Tensile Modulus 6.25 GPa
906 ksi
ISO 527
Eurotec® Tecomid® NA40 GR15 NL HS PA6.6, 15% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Tensile Modulus 6.25 GPa
906 ksi
ISO 527
Eurotec® Tecomid® NA40 GR15 NL PA 6.6 15% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Tensile Modulus 6.25 GPa
906 ksi
5 mm/min; ASTM D 638
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East)
Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu..
Copyright © lookpolymers.com All Rights Reserved