Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.0032 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
60x60x2; 300°C / MT 80°C; 600 bar; ISO 294-4
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
ISO 294-4, 2577
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber
PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds
Linear Mold Shrinkage, Flow 0.0032 cm/cm

@Time 86400 sec
0.0032 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP PDX-U-05314 PPA (Asia Pacific)
LNP* Lubricomp* PDX-U-05314 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
ISO 294-4
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFFR-4133 is a 33% glass-reinforced, halogen-free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. Th..
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hGR505 Polyphenylene Sulfide/PA Alloy
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
Sim. To ISO 294-4
DSM Arnite® TV4 461 KL (PBT+PET)-GF30
30% Glass Reinforced, Heat Stabilized, UV Stabilized, Excellent Surface Properties
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
ISO 294-4
DSM Akulon® K224-G3-FC NA99001 PA6-GF15
15% Glass Reinforced
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
ISO 2577
BASF Ultradur® S 4090 G6X High Speed 30% Glass Filled PBT
Description: Low-warpage, easy-flowing injection molding grade with 30 % glass fibers for technical parts, for which dimensional stability is very important, reduction of wall thickness (eg, e/e hou..
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
Sheet
BASF Ultradur® S 4090 GX 14% Glass Filled PBT
Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 14% of glass fibers for industrial parts with high dimensional stab..
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
ISO 294-4
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
Sim. To ISO 294-4
DSM Arnite® TV4 261 KL PBT-GF30
30% Glass Reinforced, Light Stabilized
Linear Mold Shrinkage, Flow 0.0032 - 0.0040 cm/cm
0.0032 - 0.0040 in/in
on tensile bar; SABIC Method
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East)
Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu..
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
ISO 294-4
Solvay Specialty Polymers Amodel® HFFR-4133 Polyphthalamide (PPA)  (Unverified Data**)
Amodel HFFR-4133 is a 33% glass-reinforced, halogen- free, flame retardant polyphthalamide (PPA) resin which offers enhanced processing capabilities for electrical and electronic applications. This ..
Linear Mold Shrinkage, Flow 0.0032 cm/cm
0.0032 in/in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON KEL32 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KEL32 is a compound based on Acetal Copolymer resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated.
Linear Mold Shrinkage, Flow 0.0032 cm/cm

@Time 86400 sec
0.0032 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RX06097 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX06097 is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV-Stabilized.