Polymer Property : Flexural Modulus = 769 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.30 GPa
769 ksi
Plastcom SLOVALEN PH 49 GF 30 TS PP, 30% glass fibre, mod. of mech. Properties
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...
Flexural Modulus 5.30 GPa
769 ksi
STN EN ISO 178
Plastcom SLOVALEN PH 61 GF 30 Polypropylene Homopolymer, 30% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit..
Flexural Modulus 5.30 GPa
769 ksi
STN EN ISO 178
Plastcom SLOVASTER® B1 GF 15 FRL 4 PBT reinforced with glass fibers, flame retarded
PBT reinforced with 15 % glass fiber, flame retarded with the halogen flame retardant. Anisotropy of shrinkage enables the injection molding of round, cylindrical or other hole products. Application..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Modulus 5.30 GPa

@Temperature 23.0 °C
769 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPH GF8030 PD1 VT2 PP, Glass Fiber-Reinforced, Chemically Coupled Heat Stabilized
Information provided by Polykemi AB
Flexural Modulus 5.30 GPa

@Temperature 90.0 °C
769 ksi

@Temperature 194 °F
ISO 178, ASTM D790
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
Inno-Comp INNOPOL® CS 1-5820 20% Glass-Fiber-Filled Polypropylene Homopolymer
INNOPOL® CS 1-5820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-5820 is recommended for producing in..
Flexural Modulus 5.30 GPa
769 ksi
1.3 mm/min; ASTM D790
Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced
Vyteen PC/ABS 3016 is a black 16% glass fiber reinforced Polycarbonate/ABS alloy designed for injection molding.Features: -Good processability -Balanced stiffness/resilience -High deflection temp..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, DRY
Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of..
Flexural Modulus 5.30 GPa
769 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer
LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated.
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Solvay Technyl® A216V15 15% Glass Filled Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Flexural Modulus 5.30 GPa
769 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East)
LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi.
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Solvay TECHNYL® C 402 M PA6, Conditioned
Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high ..
Flexural Modulus 5.30 GPa
769 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RFL32 PA 66
LNP* Lubricomp* RFL32 is a compound based on Nylon 66 containing 10% Glass Fiber, 15% PTFE. Added feature of this material includes: Wear Resistant.
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RX94033 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RX94033 is a compound based on PA 66 resin containing Aramide Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated.
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 (Asia Pacific)
LNP* STATKON* RFD03 is a compound based on PA 66 resin contaning Carbon Powder, Glass Fiber. Added features include: Electrically Conductive.
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East)
LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Solvay TECHNYL® A 216 V15 Black 21N PA66, 15% glass fiber, DRY
Description: Polyamide PA66, reinforced with 15% of glass fiber, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 216 V15 is used in all sectors of industry, offer..
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
Flexural Modulus 5.30 GPa
769 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RFZ22S PA 66
LNP* THERMOCOMP* RFZ22S is a compound based on Nylon 66 resin containing 10% Glass Fiber, 10% Milled Glass. Added features of this material include: Heat Stabilized.
Flexural Modulus 5.30 GPa
769 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RFZ22S PA 66 (Asia Pacific)
LNP* Thermocomp* RFZ22S is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Heat Stabilized.
Flexural Modulus 5.30 GPa
769 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East)
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178-93
Wellman Wellamid® MR409 22H-GY1 Nylon 66, 40% Mineral Reinforced
All information provided by Wellman Engineered Resins.
Flexural Modulus 5.30 GPa
769 ksi
ASTM D 790
Cossa Polimeri ESTADIENE 0835 GF Acrylonitrile Butadiene Styrene, 17% Glass Filled
ABS with 17% glass fiber reinforcementGood thermal resistance, good dimensional stability, good processabilityInformation provided by Cossa Polimeri S.r.l.
Flexural Modulus 5.30 GPa
769 ksi
DAM; ISO 178
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C40 BKB086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Celanese CELANEX 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Celanese Celanex® 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese Cor..
Flexural Modulus 5.30 GPa
769 ksi
ISO Data
BASF Ultramid® B3EG3 BK00564 15% Glass Filled PA6 (Dry)
Ultramid B3EG3 BK00564 is a 15% glass fiber reinforced, pigmented black injection molding PA6 grade for housings with enhanced impact resistance.
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East)
Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Celanese CELANEX 5202 PBT, 15% Glass Reinforced
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..