Polymer Property : Flexural Modulus = 5.30 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.30 GPa
769 ksi
STN EN ISO 178
Plastcom SLOVALEN PH 61 GF 30 Polypropylene Homopolymer, 30% Glass Fiber
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit..
Flexural Modulus 5.30 GPa
769 ksi
STN EN ISO 178
Plastcom SLOVAMID® 6 GF 25 E LS PA6 reinforced with glass fiber, UV stabilized
PA 6 grade for extrusion, reinforced with 25% glass fiber, determined for extrusion of window profile systems. Delivered in natural as well as full RAL scale color.Information Provided by Plastcom s..
Flexural Modulus 5.30 GPa
769 ksi
STN EN ISO 178
Plastcom SLOVAMID® 6 T 30 FRC 4 TS PA6 flame retarded, heat stabilized
PA 6 for injection molding, reinforced with 30% mineral filler, flame retarded with nonhalogen flame retardant, heat stabilized. Main features: flammability in accordance with UL 94 3 at 1,6 mm, glo..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Nilit FRIANYL A63 KV50 Nylon 6.6 for injection molding, 50% glass ball reinforced
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Nilit FRIANYL A63 W-GV20 Nylon 6.6 for injection molding, 20% glass fiber reinforced
Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Flexural Modulus 5.30 GPa
769 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific)
Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl..
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP DFL34 PC (Europe-Africa-Middle East)
LNP* Lubricomp* DFL34 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE.
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Celanese Celanex® 5202 PBT, 15% Glass Reinforced  (Unverified Data**)
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C4220 is a 20% glass reinforced, non FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance that combines a good processabity with a lo..
Flexural Modulus 5.30 GPa

@Temperature 23.0 °C
769 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPH GF8030 PD1 VT2 PP, Glass Fiber-Reinforced, Chemically Coupled Heat Stabilized
Information provided by Polykemi AB
Flexural Modulus 5.30 GPa

@Temperature 90.0 °C
769 ksi

@Temperature 194 °F
ISO 178, ASTM D790
Nilit Nilamid A3 H6 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H6 G6 is a 30% glass fiber reinforced NYLON 66 with a special stabilization system against hot oil and grease. As a result of this stabilization, the material has a brown nat..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Lanxess Durethan® AKV 15 H3.0 000000 Nylon 66, 15% Glass Fibers
PA 66, 15% glass fibers, injection molding, heat-ageing stabilized
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, DRY
Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Solvay Technyl® A216V15 15% Glass Filled Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Flexural Modulus 5.30 GPa
769 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS
LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi.
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Solvay TECHNYL® C 402 M PA6, Conditioned
Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high ..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Solvay TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, Conditioned
Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced po..
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RX94033 PA6.6 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RX94033 is a compound based on PA 66 resin containing Aramide Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated.
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East)
LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 5.30 GPa
769 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific)
LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced
Flexural Modulus 5.30 GPa
769 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RFZ22S PA 66
LNP* THERMOCOMP* RFZ22S is a compound based on Nylon 66 resin containing 10% Glass Fiber, 10% Milled Glass. Added features of this material include: Heat Stabilized.
Flexural Modulus 5.30 GPa
768 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® GR-4020L ABS, Glass Filled
ABS/GF material that is used in printer LBP fuserInformation provided by Samsung Cheil Industries.
Flexural Modulus 5.30 GPa
769 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS
NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color ..
Flexural Modulus 5.30 GPa
769 ksi
DAM; ISO 178
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66 Minlon 11C40 BKB086 is a 40% mineral reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Celanese Celanex® 3209HR PBT, Glass Reinforced
Celanex 3209HR is a 15% glass filled PBT that has an excellent hydrolysis resistance, mechanical properties and processability. Celanex 3209HR is non-lubricated.Information provided by Celanese Cor..
Flexural Modulus 5.30 GPa
769 ksi
ISO Data
BASF Ultramid® B3EG3 BK00564 15% Glass Filled PA6 (Dry)
Ultramid B3EG3 BK00564 is a 15% glass fiber reinforced, pigmented black injection molding PA6 grade for housings with enhanced impact resistance.
Flexural Modulus 5.30 GPa
769 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® V9235 PET (Europe-Africa-Middle East)
Valox heat stabilized, 15% Glass filled grade with mold release based on recycle PET. This grade is typically applied for business Machines applicationsThis data was supplied by SABIC-IP for the Eu..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Celanese CELANEX 5202 PBT, 15% Glass Reinforced
Celanex 5202 is a 15% glass filled polyester that features improved surface gloss and has an excellent balance of mechanical properties, processability, and color stability under heat and UV exposur..
Flexural Modulus 5.30 GPa
769 ksi
ISO 178
Polyplastic Armlen® PP GF 30-1EX Polypropylene Copolymer, 30% Glass Fiber
Information provided by PolyPlastic Group.
Copyright © lookpolymers.com All Rights Reserved