SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are longer due to limited manufacturing capability. Higher color variability and contamination risks including black specs needs to be considered before approval for use in applications.
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Moisture Absorption 0.150 %
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %
0.35 %
ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm

@Thickness 3.20 mm
0.0040 - 0.0080 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 9.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Melt Index of Compound 8.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
8.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.0 MPa
8410 psi
50 mm/min; ISO 527
60.0 MPa
8700 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 57.0 MPa
8270 psi
Type I, 50 mm/min; ASTM D638
57.0 MPa
8270 psi
50 mm/min; ISO 527
Elongation at Break 105 %
105 %
50 mm/min; ISO 527
113 %
113 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
Type I, 50 mm/min; ASTM D638
6.0 %
6.0 %
50 mm/min; ISO 527
Tensile Modulus 2.15 GPa
312 ksi
50 mm/min; ASTM D638
2.36 GPa
342 ksi
1 mm/min; ISO 527
Flexural Yield Strength 86.0 MPa
12500 psi
2 mm/min; ISO 178
91.0 MPa
13200 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.17 GPa
315 ksi
2 mm/min; ISO 178
2.21 GPa
321 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 8.52 J/cm
16.0 ft-lb/in
ASTM D256
7.41 J/cm

@Temperature -30.0 °C
13.9 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 67.0 kJ/m²
31.9 ft-lb/in²
80*10*4; ISO 180/1A
56.0 kJ/m²

@Temperature -30.0 °C
26.6 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 71.0 J

@Temperature 23.0 °C
52.4 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 64.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
72.2 µm/m-°C

@Temperature 23.0 - 80.0 °C
40.1 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 65.1 µm/m-°C

@Temperature -40.0 - 40.0 °C
36.2 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
75.5 µm/m-°C

@Temperature 23.0 - 80.0 °C
41.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
138 °C

@Thickness 3.20 mm
280 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
259 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
126 °C

@Thickness 3.20 mm
259 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 143 °C
289 °F
Rate B/50; ASTM D1525
143 °C
289 °F
Rate B/50; ISO 306
145 °C
293 °F
Rate B/120; ISO 306
Flammability, UL94 HB

@Thickness 0.750 mm
HB

@Thickness 0.0295 in
UL 94
Glow Wire Test 875 °C
1610 °F
IEC 60695-2-13
875 °C
1610 °F
IEC 60695-2-13
850 °C

@Thickness 0.800 mm
1560 °F

@Thickness 0.0315 in
IEC 60695-2-12
960 °C

@Thickness 1.00 mm
1760 °F

@Thickness 0.0394 in
IEC 60695-2-12