Polymer Property : Melt Flow = 9.2 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 9.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
SABIC Innovative Plastics GELOY FXW749SK ASA
Sparkle VisualFx ASA Resin - Weatherable
Melt Flow 9.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are..
Melt Flow 9.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
9.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific)
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color..
Melt Flow 9.2 g/10 min

@Load 10.0 kg,
Temperature 230 °C
9.2 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM-D1238
Ineos ABS Lustran® LK197 ABS, Extrusion Grade
Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e..
Melt Flow 9.2 g/10 min

@Load 5.00 kg,
Temperature 280 °C
9.2 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL HN731A PPE+PS
PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine..
Melt Flow 9.2 g/10 min

@Load 5.00 kg,
Temperature 280 °C
9.2 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..
Melt Flow 9.2 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.2 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Diamond Polymers ASA M-523
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Melt Flow 9.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Diamond Polymers DIAMALOY GLY FXW749 Sheet Extrusion Grade, Sparkle/Pearlescence