Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.52 J/cm | 16.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are.. |
|||
Izod Impact, Notched | 8.52 J/cm | 16.0 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |