Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 56.0 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
26.6 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² @Temperature -30.0 °C |
26.6 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are.. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² | 26.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² | 26.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² | 26.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² | 26.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® SD1278 PC Copolymer (Asia Pacific) Lexan* SD1278 polycarbonate (PC) siloxane copolymer resin is a transparent extrusion grade for food contact applications for sheet extrusion. This resin offers extreme low temperature (-40 °C) .. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² @Temperature -30.0 °C |
26.6 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² | 26.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY D2000 PC (Asia Pacific) LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² | 26.6 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRILOY D2000AXH PC LNP LUBRILOY* D2000AXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² @Temperature 23.0 °C |
26.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Lubriloy D2000XXH PC LNP LUBRILOY* D2000XXH is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated, Healthcare.This data was supplied.. |
|||
Izod Impact, Notched (ISO) | 56.0 kJ/m² @Temperature -50.0 °C |
26.6 ft-lb/in² @Temperature -58.0 °F |
|
Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2553 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and impact strength with excellent stiffness for hou.. |
|||
Izod Impact, Notched (ISO) | 56.0 - 56.0 kJ/m² @Temperature -50.0 - -50.0 °C |
26.6 - 26.6 ft-lb/in² @Temperature -58.0 - -58.0 °F |
Average value: 56.0 kJ/m² Grade Count:1 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |