Mechanical Properties Metric English Comments
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are..
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Asia Pacific)
7 MFR LEXAN HFD Copolymer
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer (Europe-Africa-Middle East)
7 MFR LEXAN HFD Copolymer
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Asia Pacific)
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1034 PC Copolymer (Europe-Africa-Middle East)
7 MFR LEXAN HFD Copolymer UV-stabilized, available in transparent colors only
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Lexan® HPS4 PC
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable...
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Lexan® HPS4 PC (Asia Pacific)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable...
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
ISO 179/2C
SABIC Innovative Plastics Lexan® HPS4 PC (Europe-Africa-Middle East)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable...
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific)
Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color..
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
SABIC Innovative Plastics Lexan® HFD1014 PC Copolymer
7 MFR LEXAN HFD Copolymer
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
ISO 179
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP
SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac..
Charpy Impact, Notched 8.20 J/cm²
39.0 ft-lb/in²
Arkema Group Orgalloy® LT 4060IH Flexible Nylon Alloy (Conditioned)
Very flexible polyamide alloy: easy to process, low moisture absorption, good mechanical properties at low temperature. Demonstrate a good balance of properties eg, high flexibility (200 MPa), good ..