Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.15 GPa | 312 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 1173X PC Copolymer (Europe-Africa-Middle East) Lexan* 1173X polycarbonate (PC) resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-30 C) ductility in combination with high flow characteristics an.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Asia Pacific) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1434 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade and is UV stabilized. This resin offers extreme low temperature (-40 C), exhibits exce.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer (Asia Pacific) Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXE1414 PC Copolymer Lexan* FXE1414 polycarbonate (PC) siloxane copolymer resin is a special effects fluorescent, medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductil.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Asia Pacific) 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7647 PC (Europe-Africa-Middle East) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque onlyThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Asia Pacific) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 4301 PPC+PC Lexan 4301 is a high heat resistant poly (ester) carbonate resin for injection moldingThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL1414H PC Copolymer Opaque PC-Siloxan copolymer with excellent processability. Medium flow, extreme low temperature ductile. Enhanced hydrolytic stability. Only available in black color. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXRL0682 PC Copolymer 18 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Tensile Modulus | 2.15 GPa @Thickness 3.20 mm |
311 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 |
LG Chemical LG-709 ABS, Low Gloss, Super High Heat Resistance Information Provided by LG Chem |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 2.15 GPa | 312 ksi | ISO 527-1/-2 |
Covestro Makroblend® KU 2-7912/4 Polycarbonate + PBT, Impact Grade ISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesideal for painted applicationsunreinforcedPreprocessingMax. Water content |
|||
Tensile Modulus | 2.15 GPa @Thickness 3.20 mm |
311 ksi @Thickness 0.126 in |
1mm/min; ASTM D638 |
LG Chemical LI923 Extrusion ASA Description: Good Weatherability, High RigidityApplication: Communication Instrument Cover, Cable Connecting Cover, Door PanelCAS: 26299-47-8Information provided by LG Chemical |