Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 8.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polykemi AB POLYasa 1614F UV-resistant ASA Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE ZC100 D40 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF8030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin. Glass transition Temp. (Tg) of 247°C. Global Food Contact Approval. Resin is subject to Commerce Control Laws U.S. 15CFR Chapter VII, Part 774 and .. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC T8040 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PP HIP8040F VT2 Polypropylene, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH B8075 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 300 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Europe-Africa-Middle East) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 280 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL N190 PPE+HIPS (Europe-Africa-Middle East) NORYL N190 is an unfilled, flame retardant material with a Vicat B/120 of 105°C according ISO 306. NORYL N190 is V0 at 1.52 mm and 5VA at 3.12 mm according UL94 and halogen free according VDE/DIN.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM AUT230 PEI Transparent polyetherimide (Tg 247 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 265 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Melt Index of Compound | 8.0 g/10 min @Temperature 230 °C |
8.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
Melt Index of Compound | 8.0 g/10 min | 8.0 g/10 min | Condition L; ASTM D1238 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Melt Index of Compound | 8.0 g/10 min | 8.0 g/10 min | Condition L; ASTM D1238 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Melt Index of Compound | 8.0 g/10 min @Temperature 230 °C |
8.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ S6002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
Melt Index of Compound | 8.0 g/10 min @Temperature 230 °C |
8.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
Melt Index of Compound | 8.0 - 25 g/10 min | 8.0 - 25 g/10 min | ASTM D1238, ISO 1133 |
EPICHEM Epicarb PC BLACK IQ Polycarbonate Characteristics: good fluidity, good impact, industrial quality |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow 722 Linear Low Density Polyethylene (LDPE) DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific) Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |