SABIC Innovative Plastics LNP Thermocomp MB006SU PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp MB006SU PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* MB006SU is a compound based on Polypropylene resin containing Glass Bead. Added features include: Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 22.0 MPa
3190 psi
50 mm/min; ISO 527
Tensile Strength, Yield 25.0 MPa
3630 psi
50 mm/min; ISO 527
Elongation at Yield 4.8 %
4.8 %
50 mm/min; ISO 527
Tensile Modulus 2.10 GPa
305 ksi
1 mm/min; ISO 527
Flexural Yield Strength 42.0 MPa
6090 psi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 104 µm/m-°C

@Temperature 23.0 - 60.0 °C
57.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 114 µm/m-°C

@Temperature 23.0 - 60.0 °C
63.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °C
151 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af