Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible A7000 Polyvinyl Chloride, Flexible (PVC, Flexible)
Interior compound used primarily in transparent applications. This product is registered under UL 94 HB specifications @ 3.0 and 1.5 mm. thickness and all colors.Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible A75M1 Trans 9000 Polyvinyl Chloride, Flexible (PVC, Flexible)
This compound is certified for fuel hose applications(R1 Type B Class 1)under SAE J 1527 requirements.Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible B65B0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 2.00 mm
0.019 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer  (Unverified Data**)
Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided..
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 2.00 mm
0.019 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ASTM D955
Celanese Celcon® MC270 POM, Mineral Reinforced  (Unverified Data**)
Celcon® MC270 is a mineral coupled acetal copolymer designed for applications requiring improved stiffness, lower mold shrinkage and reduced warpage while maintaining the mechanical performance cha..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4
Celanese Hostaform® C 27021 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with high flowInformation provided by Celanese
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4
Celanese Hostaform® C 9021 AS POM, Specialty  (Unverified Data**)
POM copolymerAntistatic gradeInformation provided by Celanese
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ASTM D955
PolyOne Geon™ Vinyl Flexible B65U0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4
Celanese Hostaform® LU-02XAP® POM, UV Resistant  (Unverified Data**)
Hostaform® acetal copolymer grade LU-02 XAP® is UV stabilized material displaying a reduced gloss over standard UV acetal grades similar to LU-02. However, Hostaform® LU-02XAP® has lower volati..
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 3.17 mm
0.019 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PP 0096 S2 LE Polypropylene
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 3.17 mm
0.019 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Luriblend® TPX-PA6/6-95001
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Solvay TECHNYL® A 217 PA66, DRY
Description: TECHNYL ® A 217 is an unreinforced polyamide 66, heat stabilized, standard viscosity, for injection molding. It is available in black color.Benefits: This product offers all the prim..
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 3.17 mm
0.019 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® LDPE 0098 S LE
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforAdditive: Heat StabilizerFeatures: Low ExtractablesInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Solvay TECHNYL® 2710IR PA66, DRY
Description: TECHNYL® 2710 IR is an unfilled polyamide 6.6, impact modified, for injection molding. The product is available in natural color, and in colors on request.Benefits: This product, use..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
24 hours + 30 min at 93°C
Teknor Apex TEKRON® 4300LM-P88-1 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Linear Mold Shrinkage, Flow 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ISO DIS 294-4
Wellman Wellamid® XT1482-BK High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4 2577
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® 511DP BK402 Acetal (POM)  (Unverified Data**)
Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4 2577
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4 2577
DuPont Performance Polymers Hytrel® HTR8730 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Viscosity Polyester Elastomer with Excellent Mechanical Properties at Elevated Temperatures Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4
Barlog Plastics KEBAFLEX SG 75 A.1 black TPE-S, Shore A75, black
TPE-SInformation provided by BARLOG plastics GmbH.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Celanese Celanex® 2000 Polyester (PBT)
High melt flowInformation provided by Celanese Corporation.
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 2577
BASF Ultraform® N2640 Z2 POM + PUR
Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS..
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 2.00 mm
0.019 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt..
Linear Mold Shrinkage, Flow 0.019 cm/cm

@Thickness 2.00 mm
0.019 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Delrin® 588P NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 588P NC010 is a medium viscosity acetal homopolymer resin for injection molding. It has good thermal stability, and modifications for more precise molding (reduced warpage, good dimensiona..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ASTM D955
Celanese Celcon® MC90 POM, Mineral Reinforced  (Unverified Data**)
Celcon® acetal copolymer grade MC90 is a mineral reinforced grade offering low warp, improved dimensional stability, improved stiffness, improved practical impact and retention of other base resin ..
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4
Celanese Hostaform® S 27063 POM, Impact Modified  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POM-HI,Easy flowing elastomer-containing injection molding grade, moderate toughnessInformation provided by Celanese
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
ISO 294-4
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified  (Unverified Data**)
Preliminary Data SheetImpact modified, improved modulus and weld line, low emissionInformation provided by Celanese
Linear Mold Shrinkage, Flow 0.019 cm/cm
0.019 in/in
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY
Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit..