Material Notes:
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Moisture Absorption 0.100 %
0.100 %
50% RH, 24 hrs; ASTM D570
0.140 %
0.140 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0039 cm/cm

@Time 86400 sec
0.0039 in/in

@Time 24.0 hour
ISO 294
0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D955
0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 64.0 MPa
9280 psi
ASTM D638
64.0 MPa
9280 psi
ISO 527
Elongation at Break 3.2 %
3.2 %
ISO 527
3.6 %
3.6 %
ASTM D638
Tensile Modulus 3.45 GPa
500 ksi
50 mm/min; ASTM D638
3.75 GPa
544 ksi
1 mm/min; ISO 527
Flexural Strength 103 MPa
14900 psi
ISO 178
116 MPa
16800 psi
ASTM D790
Flexural Modulus 3.51 GPa
509 ksi
ASTM D790
3.52 GPa
511 ksi
ISO 178
Izod Impact, Notched 0.230 J/cm
0.431 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.50 J/cm
10.3 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 1.00 J
0.738 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
52.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.0 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 52.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
52.4 µm/m-°C

@Temperature -40.0 - 40.0 °C
29.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
86.0 °C

@Thickness 3.20 mm
187 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
82.0 °C

@Thickness 3.20 mm
180 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.70 mm
V-0

@Thickness 0.0669 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257
Users viewing this material also viewed the following: