Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 36.0 - 50.0 kJ/m² @Temperature -25.0 - 120 °C |
17.1 - 23.8 ft-lb/in² @Temperature -13.0 - 248 °F |
Average value: 41.3 kJ/m² Grade Count:1 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific) LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66 LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC (Asia Pacific) LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON JX89626 PES LNP* STAT-KON* JX89626 is a compound based on Polyethersulfone containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP KFZ24XXP Acetal Copoly LNP* THERMOCOMP* KFZ24XXP is a compound based on Acetal Copolymer resin containing 20% Glass Fiber, 10% Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled, Inter.. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RF0049SP PA 66 LNP* THERMOCOMP* RF0049SP is a compound based on Nylon 66 containing 20% Glass Fiber. Added features of this grade include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66 LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² @Temperature -30.0 °C |
17.1 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® SHF4960 PBT Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² @Temperature 23.0 °C |
17.1 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 36.0 kJ/m² | 17.1 ft-lb/in² | ISO 180/1U |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Izod Impact, Unnotched (ISO) | 36.0 - 50.0 kJ/m² @Temperature -25.0 - 120 °C |
17.1 - 23.8 ft-lb/in² @Temperature -13.0 - 248 °F |
Average value: 41.3 kJ/m² Grade Count:1 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |