Polymer Property : Izod Impact, Unnotched (ISO) = 17.1 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 36.0 - 50.0 kJ/m²

@Temperature -25.0 - 120 °C
17.1 - 23.8 ft-lb/in²

@Temperature -13.0 - 248 °F
Average value: 41.3 kJ/m² Grade Count:1
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Izod Impact, Unnotched (ISO) 36.0 kJ/m²

@Temperature 23.0 °C
17.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp EL004 PEI
LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas..
Izod Impact, Unnotched (ISO) 36.0 kJ/m²

@Temperature 23.0 °C
17.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific)
LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac..
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP RL004 PA 66
LNP* LUBRICOMP* RL004 is a copmpound based on Nylon 66 resin containing 20% PTFE. Added feature of this grade includes: Wear Resistant.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC
LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing 20% Glass Fiber, Proprietary Lubricant. Added features include: Flame Retardant.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRILOY DF2041 PC (Asia Pacific)
LNP LUBRILOY* DF2041 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant, Glass Fiber. Added features of this material include: Flame Retardant.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DD0001 PC
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON JX89626 PES
LNP* STAT-KON* JX89626 is a compound based on Polyethersulfone containing Proprietary Fillers. Added feature of this material is: Electrically Conductive.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP KFZ24XXP Acetal Copoly
LNP* THERMOCOMP* KFZ24XXP is a compound based on Acetal Copolymer resin containing 20% Glass Fiber, 10% Milled Glass. Added features of this material include: Low Warpage, Chemically Coupled, Inter..
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RF0049SP PA 66
LNP* THERMOCOMP* RF0049SP is a compound based on Nylon 66 containing 20% Glass Fiber. Added features of this grade include: Flame Retardant, Heat Stabilized.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP RFB66 PA 66
LNP* THERMOCOMP* RFB66 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 30% Glass Bead.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²

@Temperature -30.0 °C
17.1 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics Valox® SHF4960 PBT
Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²

@Temperature 23.0 °C
17.1 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Thermocomp 2C004
LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup..
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE
LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 36.0 kJ/m²
17.1 ft-lb/in²
ISO 180/1U
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8..
Izod Impact, Unnotched (ISO) 36.0 - 50.0 kJ/m²

@Temperature -25.0 - 120 °C
17.1 - 23.8 ft-lb/in²

@Temperature -13.0 - 248 °F
Average value: 41.3 kJ/m² Grade Count:1
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc..