Mechanical Properties Metric English Comments
Tensile Modulus 3.75 GPa
544 ksi
ISO 527-1/-2
Quadrant EPP Ketron® TX PEEK + solid lubricant, extruded (ISO Data)
This member of the Ketron PEEK family has been developed especially for the food industry. Like Ketron PEEK-1000, this new internally lubricated material has a food contact compliant composition, bu..
Tensile Modulus 3.75 GPa
544 ksi
Radici Radilon® S RV150 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Tensile Modulus 3.75 GPa
544 ksi
ISO 527-2
Pasargad Polymer Peyvand Pasamid 3P-H1000B Nylon 6
Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co
Tensile Modulus 3.75 GPa
544 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD0001 PC
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant.
Tensile Modulus 3.75 GPa
544 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Tensile Modulus 3.75 GPa
544 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East)
LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive.
Tensile Modulus 3.75 GPa

@Temperature 23.0 °C
544 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® FR7025V0F NC010 Nylon 66  (Unverified Data**)
Zytel® FR7025V0F NC010 is a flame retardant polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuPont Performance..
Tensile Modulus 3.75 GPa
544 ksi
ISO 527
Eurotec® Tecomid® NA40 NL FA 50 PA 6.6 unreinforced, UL94 V0, halogen/phosphorus free
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Tensile Modulus 3.75 GPa
544 ksi
ISO 527
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural
Information provided by Eurotec®
Tensile Modulus 3.75 GPa
544 ksi
ISO 527
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Tensile Modulus 3.75 GPa
544 ksi
ISO 527
Eurotec® Tecomid® NB40 NL XA 20 PA 6 unreinforced, UL94 V0
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Tensile Modulus 3.75 GPa
544 ksi
ISO 527
Eurotec® Tecomid® NA40 MR15 NL IL PA 6.6 15% mineral reinforced, impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Tensile Modulus 3.75 GPa
544 ksi
ISO 527
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural