Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.50 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
10.3 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Izod Impact, Unnotched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Cycoloy® C4220K PC+ABS (Asia Pacific) Cycoloy* C4220K resin is an injection moldable 20% glass reinforced non FR PC-ABS.
Key features include improved Knit Line strength, good flow, excellent strength & rigidity, heat resistance & hyd.. |
|||
Izod Impact, Unnotched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp DFL329EF PC LNP LUBRICOMP* DFL329EF is a compound based on Polycarbonate resin containing Flame Retardant, Glass Fiber, PTFE. Added features of this material include: Flame Retardant.This data was supplied by .. |
|||
Izod Impact, Unnotched | 5.50 J/cm @Thickness 3.18 mm |
10.3 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® OFL-4036 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Unnotched | 5.50 J/cm @Thickness 3.18 mm |
10.3 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® UF-1006 FR HS LEX BK8-115 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Features: Heat Stabilized, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many L.. |
|||
Izod Impact, Unnotched | 5.50 J/cm @Thickness 3.18 mm |
10.3 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Lubricomp® EFL-4036 UFE Polyetherimide, Glass Fiber Reinforcement, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Branched (Asia Pacific) LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched (Europe-Africa-Middle East) LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS (Asia Pacific) LNP* Lubricomp* OFL36A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT Health care grade, PTFE and silicone lubricated |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Asia Pacific) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DD0001 PC (Europe-Africa-Middle East) LNP STAT-KON* DD0001 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC LNP* STAT-KON* DE0039 is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Flame Retardant. Electrically Conductive. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Unnotched | 5.50 J/cm @Temperature -30.0 °C |
10.3 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Asia Pacific) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Unnotched | 5.50 J/cm @Temperature -30.0 °C |
10.3 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Valox® ENH4550 PBT (Europe-Africa-Middle East) 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Unnotched | 5.50 J/cm @Temperature 23.0 °C |
10.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp GF003 PSU LNP THERMOCOMP* GF003 is a compound based on Polysulfone resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UF0069S PPA LNP THERMOCOMP* UF0069S is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL GFN2 PPE+HIPS (Asia Pacific) PPE+PS blend. 20% Glass reinforced. FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump.. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DE0039 PC (Asia Pacific) LNP* Stat-kon* DE0039 is a compound based on Polycarbonate resin containing Flame Retardant, Carbon Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 113 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DFL329 PC LNP LUBRICOMP* DFL329 is a compound based on Polycarbonate resin containing 10% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Izod Impact, Unnotched | 5.50 J/cm | 10.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP JF006EXZ PES LNP* THERMOCOMP* JF006EXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |