Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.28 g/cc | 0.0462 lb/in³ | |
Plastcom SLOVAMID 6 NG1 GF 20 HLS PA6, 20% glass fibre, combined stability FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre, heat and wheather stabilized. Stabilized against hydrolisys. Good surface finisch. Scratch resistent.Packaging, tra.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC LNP LUBRICOMP* DL003 is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | DIN 53479; ASTM D792 |
Kolon KOPA® KN133G20 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RX88514 PA 66 LNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). AddedLNP LUBRICOMP* RX85514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). A.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM CRS5011R PEI Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU1004 PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM HU1004 PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON TX06488NTX1 PU LNP* STAT-KON* TX06488NTX1 is a compound based on Polyurethane resin containing Proprietary Filler(s). Added features of this grade are: Execllent Ductility, Electrically Conductive. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
SABIC Innovative Plastics ULTEM 9090 PEI (Europe-Africa-Middle East) Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
Techmer ES Electrablend® PA6/6 03004 GF20 Carbon/20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement/Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Lubricant, Impact Modifier and Heat StabilizerFeatu.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN® EG106 ABS Inherently Static Dissipative and Glass Fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plastx.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
Polyram PlusTek PA350M4 Nylon 6.6 for Injection Molding, 20% Mineral Reinforced 20% Mineral Reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GFX1356-BK01 20% Glass Fiber Reinforced, Lubricated Nylon 6 Description: Glass Fiber Reinforced, Lubricated Nylon 6Information provided by Wellman. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | Resin |
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/G1094/1000 Fiber: T800H 6K, 5H Satin weave, 290 g/m2Information provided by HexCel |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
Covestro Bayblend® FR 3021 Polycarbonate + ABS, Mineral Filled 15 % mineral filledinjection molding gradeincreased stiffnesstensile modulus = 4800 MPaVicat/B 120 temperature = 98 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame ret.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | |
DuPont Performance Polymers Crastin® LW9030 NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030 NC010 is a 30% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 55 Flexible PVC, Injection Molding for Footwear Tennis shoes |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 8016 Flexible PVC, Injection Molding for Footwear Technical items for footwear |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds FRT 91 Flexible PVC, Insulation Telephone cables |
|||
Density | 1.28 - 1.32 g/cc | 0.0462 - 0.0477 lb/in³ | ISO R 1183 |
Fainplast Compounds GS 7022 Flexible PVC, Injection Molding for Footwear Soles |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | |
Arkema Group Orgalloy® R 6030 Nylon 6 Alloy, 30% Glass fiber (Conditioned) Rigid polyamide 6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents).Special 30% glass fiber reinforced for overmolding with modified PP.ISO data provided by th.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | ISO 1183 |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Conditioned, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Density | 1.28 g/cc | 0.0462 lb/in³ | (Dry) |
BASF Capron® GR20 HS 20% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron GR20 HS is a heat stabilized 20% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest.. |
|||
Density | 1.28 - 1.61 g/cc | 0.0462 - 0.0582 lb/in³ | Average value: 1.43 g/cc Grade Count:102 |
Overview of materials for Polycarbonate, Glass + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass + PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Density | 1.28 g/cc @Temperature 121 °C |
0.0463 lb/in³ @Temperature 250 °F |
Dry Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M77HS Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or spre.. |