Resin Technology Group 1105 Oxy-Bond™ Two-Component Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group 1105 Oxy-Bond™ Two-Component Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to match a variety of specific application parameters, including MIL-APPROVED. Custom designed bonding products and expert technical assistance are always available.Resin Technology Group 1105 Oxy-Bond™ Two-Component Epoxy AdhesiveHigh performance, medium viscosity, 5 minute fixture adhesive.
Physical Properties Metric English Comments
Viscosity 15000 cP
15000 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 23.0 °C
1.00 hour

@Temperature 73.4 °F
Pot Life 3.0 - 5.0 min
3.0 - 5.0 min
3.0 - 5.0 min
3.0 - 5.0 min