Material Notes:
Scotch® Transparent Film Tape 605 is designed for various light-duty packaging applications such as attaching, mending, gift wrapping, holding and L-Clips. This product offers good performance over broad temperature ranges; specifically in cold and damp applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 40.6 microns
1.60 mil
Backing; ASTM D3652
63.5 microns
2.50 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Elongation at Break 57 %
57 %
ASTM D3759
Peel Strength 0.29582 kN/m
1.6875 pli
Adhesion to Steel; ASTM D3330
Film Tensile Strength at Break, TD 6.11 MPa
886 psi
ASTM D3759
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive acrylic
Appearance Clear