| Category | Polymer , Thermoplastic , Polypropylene (PP) |
| Manufacturer | LyondellBasell |
| Trade Name | Pro-fax |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | LyondellBasell Pro-fax SD242 Polypropylene Impact Copolymer.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792B |
| Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 28.0 MPa | 4060 psi | ASTM D638 |
| Elongation at Yield | 5.0 % | 5.0 % | ASTM D638 |
| Flexural Modulus | 1.40 GPa | 203 ksi | 1% secant at 0.05 in/min; ASTM D790A |
| Izod Impact, Notched | 0.700 J/cm | 1.31 ft-lb/in | ASTM D256A |
| Impact Test | 20.0 J @Temperature 5.00 °C |
14.8 ft-lb @Temperature 41.0 °F |
Montell drop weight impact strength |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 70.0 °C | 158 °F | ASTM D648 |
| UL RTI, Mechanical with Impact | 65.0 °C | 149 °F | Minimum thickness of 0.059 inches. |
| Flammability, UL94 | HB | HB | Minimum thickness of 0.059 inches. |