Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 15000 cP | 15000 cP | Thixotropic |
ND Industries 240 Structural Adhesive Excellent impact and solvent resistance |
|||
Viscosity | 15000 - 20000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
15000 - 20000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK2.1° |
Gwent Electronic Materials D2090126D2 Black Solder mask Dielectric This product has been designed as a solder mask dielectric for use at high temperatures. It has been tested at 250°C and was proved to be stable for 4 weeks. Screen Printing Equipment: semi-autom.. |
|||
Viscosity | 15000 - 30000 cP @Temperature 25.0 °C |
15000 - 30000 cP @Temperature 77.0 °F |
|
Lucite International Colacryl ® TS1631 Acrylic Solution Resin Acrylic copolymer with reactive groupsA highly flexible resin with good handle. It exhibits good adhesion, resistance to ageing and light stability.Suggested Use: Coating and lamination of nylon and.. |
|||
Viscosity | 15000 - 35000 cP | 15000 - 35000 cP | |
Huntsman Matrimid 5292B Resin Comments/Applications: Max Color is 6. 0,0' - Diallyl bisphenol A hardener, brown liquid. Use with Matrimid 5292A to optimize processing, toughness and performance.Data provided by Ciba Specialty .. |
|||
Viscosity | 15000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
15000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7030-1000 TPE Product Description: StarMediflex P 7030-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
Viscosity | 15000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
15000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-85-1000 TPE Product Description: StarXTRUDE XTR-85-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |
|||
Viscosity | <= 15000 cP | <= 15000 cP | #3 SP @ 12 rpm; RP-0596 |
Solvay MIRASHEEN® CP-820 Surfactant Description: New generation of ready to use, cost effective liquid pearl concentrate. A pumpable liquid that readily blends into formulated shampoos, liquid hand soaps, shower gels and related produ.. |
|||
Viscosity | 15000 - 25000 cP | 15000 - 25000 cP | Part A |
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance.. |
|||
Viscosity | 15000 cP | 15000 cP | dynamic |
Dow Corning SILASTIC® 9252/150P A&B KIT 35 Durometer, 2-part, 10 to 1 mix, translucent, Fabric Coating grade, Liquid Silicone RubberInformation provided by Dow Corning |
|||
Viscosity | 15000 - 32000 cP @Temperature 23.0 °C |
15000 - 32000 cP @Temperature 73.4 °F |
10 rpm |
Epoxy Technology EPO-TEK® B9021-6 Epoxy Paste Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta.. |
|||
Viscosity | 15000 - 18000 cP @Temperature 23.0 °C |
15000 - 18000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® E2101 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E2101 is a two component, thixotropic, electrically conductive adhesive. It may be used for circuit assembly and semiconductor applications. Advantages & Application .. |
|||
Viscosity | 15000 cP | 15000 cP | |
Cotronics Duralco™ 120 500°F Silver Filled Epoxy, Electrically Conductive Contains over 70% ultra fine silver to provide excellent electrical conductivity. Cures at room temperature.>Applications: ideal for use where maximum conductivity is required. |
|||
Viscosity | 15000 cP | 15000 cP | |
Cotronics Duralco™ 128 500°F (260°C) Ceramic Filled Epoxy Ceramic filled, electrically resistant adhesive and potting compound. The ceramic fillers provide both high thermal conductivity and high dielectric strength. Cures at room temperature. Curing ca.. |
|||
Viscosity | 15000 cP | 15000 cP | Mixed |
Armstrong A-2/H20 Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |
|||
Viscosity | 15000 cP | 15000 cP | |
ACC MM906 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Viscosity | 15000 cP | 15000 cP | catalyzed with QM CAT RED 3 |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Viscosity | 15000 cP @Temperature 177 °C |
15000 cP @Temperature 350 °F |
Typical |
Bostik 2124 Flexible, Long Open Time EVA Glue Stick Bostik 2124 Flexible, Long Open Time EVA Glue StickFlexible. Long open time for most difficult substrates. |
|||
Viscosity | 15000 - 25000 cP | 15000 - 25000 cP | ASTM D562 |
Asia Technology Pioneers CAN 102 Acrylic Hi-Compound Resin Description: ACN 102 is hi-tech compounded Acrylic Resin. This hi-composite is produced by Nano-Technology and used widely in paint and Coating industryAdvantages:High abrasion and corrosion resista.. |
|||
Viscosity | 15000 cP | 15000 cP | |
Cotronics Duralco™ 126 450°F (230°C) Silver Filled Epoxy Two component, silver-filled epoxy for hi-power applications. Cures with mild heat. |
|||
Viscosity | 15000 cP | 15000 cP | Part B, RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP1026 Clear Epoxy Adhesive Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Viscosity | 15000 cP | 15000 cP | Part B, RVT, #5, 2.5 rpm; TM R050-12 |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Viscosity | 15000 cP | 15000 cP | Part A, RVT, #5, 2.5 rpm; TM R050-12 |
Resinlab® EP1199 Black Unfilled Epoxy Adhesive Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Viscosity | 15000 - 20000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
15000 - 20000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK2.1° |
Gwent Electronic Materials D2090124D2 Green Solder mask Dielectric This product has been designed as a solder mask dielectric for use at high temperatures. It has been tested at 250°C and was proved to be stable for 12 weeks. Screen Printing Equipment: semi-automa.. |
|||
Viscosity | 15000 cP @Shear Rate 10994 1/s, Temperature 210 °C |
15000 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarCLEAR CLR-1045 TPE Product Description: StarCLEAR CLR-1045 is an easy processing TPE designed for injection molding. Soft and ultra clear TPEs specifically targeted to medical, consumer and sporting goods market. Feat.. |