Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Resin Technology Group 1105 Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Resin Technology Group 1105 Oxy-Bond™ Two-Component Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Small Mass |
Resin Technology Group TIGA 101-EX Five-Minute Epoxy Adhesive 1 part resin to 1 part hardener.TIGA 101-EX is an exceptional epoxy formulation, recommended for lower temperature or wet industrial bonding applications where fast curing is required. This clear, t.. |
|||
Pot Life | 3.0 - 4.0 min | 3.0 - 4.0 min | Time before parts must be mated |
Lord Adhesives 510 Fast Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Pot Life | 3.0 - 4.0 min | 3.0 - 4.0 min | Time before parts must be mated |
Lord Adhesives 513 Fast Cure, Non-Sagging Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Time before parts must be mated |
Lord Adhesives 7545B Two-Component, Equal-Mix, Non-Sag Urethane Adhesive Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | 100 gram mass |
Master Bond EP21LVSP6 Two component epoxy for bonding, sealing, coating and encapsulating Product Description: Master Bond EP21LVSP6 is a two component epoxy compound for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at room temperature or more ra.. |
|||
Pot Life | 3.0 min @Temperature 24.0 °C |
3.0 min @Temperature 75.2 °F |
gel time, 200g; ASTM 2471-71 |
BCC Products DP-11-90 Urethane Casting DP-11-90 is an unfilled, low viscosity, quick setting two component urethane system. An easy to use 1 to 1 mix ratio (Part A/Part B), DP-11-90 offers the user a 3 minute working time with parts demo.. |
|||
Pot Life | 3.0 min @Temperature 24.0 °C |
3.0 min @Temperature 75.2 °F |
gel time, 200g; ASTM 2471-71 |
BCC Products BC 8400 Urethane Casting BC8400 is an unfilled, low viscosity, quick setting two component urethane system. When properly cured, BC 8400 will exhibit high impact strength and yield thermoplastic-like parts. Some features i.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Mass: 25g; TM R050-19 |
Resinlab® EP1026 Clear Epoxy Adhesive Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Mass: 50g; TM R050-19 |
Resinlab® EP1026HP Epoxy Adhesive Resinlab™ EP1026HP is a high performance fast setting epoxy adhesive designed for bonding metals, ceramics, glass and most plastics. This product gives good resistance to water salt spray, inorgan.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Mass: 50g; TM R050-19 |
Resinlab® EP1026R Rubber Modified Epoxy Adhesive Resinlab™ EP1026R is a two part unfilled rubber modified epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free .. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Loctite® Durabond® E-00CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Loctite® Durabond® E-00NS Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | |
Loctite® Durabond® E-05CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 3.0 - 5.0 min | 3.0 - 5.0 min | Mass: 25g; TM R050-19 |
Resinlab® EP1026 Black Epoxy Adhesive Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in .. |