Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® S CV300 (cond.) Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® S CV300 (cond.) Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
(Dry)
Water Absorption 9.0 %
9.0 %
initially dry
Moisture Absorption at Equilibrium 2.7 %
2.7 %
initially dry
Viscosity Measurement 140
140
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.0 MPa
5080 psi
Elongation at Break 40 %
40 %
Nominal
Elongation at Yield 15 %
15 %
Tensile Modulus 2.50 GPa
363 ksi
Charpy Impact Unnotched 3.50 J/cm²

@Temperature -30.0 °C
16.7 ft-lb/in²

@Temperature -22.0 °F
4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.210 J/cm²

@Temperature -30.0 °C
0.999 ft-lb/in²

@Temperature -22.0 °F
0.410 J/cm²

@Temperature 23.0 °C
1.95 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Comparative Tracking Index 550 V
550 V