Arlon TC350 Glass, PTFE and Micro-Dispersed Ceramic

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon TC350 Glass, PTFE and Micro-Dispersed Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 2.30 g/cc
0.0831 lb/in³
Water Absorption 0.050 %
0.050 %
Outgassing - Total Mass Loss 0.010 %
0.010 %
Collected Volatile
0.020 %
0.020 %
Total Mass Loss
Mechanical Properties Metric English Comments
Peel Strength 1.23 kN/m
7.00 pli
Thermal Properties Metric English Comments
CTE, linear 7.00 µm/m-°C
3.89 µin/in-°F
x direction
7.00 µm/m-°C
3.89 µin/in-°F
y direction
CTE, linear, Transverse to Flow 23.0 µm/m-°C
12.8 µin/in-°F
z direction
Thermal Conductivity 1.03 W/m-K
7.15 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1.00e+10 Hz
3.5

@Frequency 1.00e+10 Hz
3.5

@Thickness 0.127 mm
3.5

@Thickness 0.00500 in
3.5

@Thickness 6.35 mm
3.5

@Thickness 0.250 in
Dissipation Factor 0.0020

@Frequency 1.00e+10 Hz
0.0020

@Frequency 1.00e+10 Hz
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -9