Polymer Property : Charpy Impact, Notched = 0.210 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.210 J/cm²

@Temperature -20.0 °C
0.999 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVASTER® B1 GF 10 FRX 5 PBT reinforced with 10% glass fibre, with flame retardant
Features: PBT with the content of 10 % chemically bound glass fibre and with the halogen freeflame retardant. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other ho..
Charpy Impact, Notched 0.210 J/cm²

@Temperature 23.0 °C
0.999 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVAMID 6 GF 5 PA6, 5% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 5% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and ..
Charpy Impact, Notched 0.210 J/cm²

@Temperature -30.0 °C
0.999 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Inno-Comp INNOPOL® CS 1-3130 30% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-3130 is a 30% talc-filled polypropylene homopolymer compound /PP-H TD30 (ISO 1043)/. This grade is available in natural and custom colored form as well.INNOPOL® CS 1-3130 is reco..
Charpy Impact, Notched 0.210 J/cm²

@Temperature -20.0 °C
1.00 ft-lb/in²

@Temperature -4.00 °F
Complete Break; ISO 179
ExxonMobil Exxtral™ CMW 203 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by high flow and designed for automotive interior applications such as door panel linings and other low pressure back mo..
Charpy Impact, Notched 0.210 J/cm²

@Temperature -30.0 °C
0.999 ft-lb/in²

@Temperature -22.0 °F
Radici Radilon® S CV300 (cond.) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.