A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer

Category Polymer , Thermoplastic
Manufacturer A. Schulman, Inc.
Trade Name SCHULAFLEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples. ApplicationSF230 is ideally suited for products requiring a soft feel.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.882 g/cc
0.882 g/cc
ASTM D792
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
F50; ASTM D1693
Melt Index of Compound 35 g/10 min
35 g/10 min
2.16/190; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 27
27
15 sec delay; ASTM D2240
Tensile Strength, Yield 3.10 MPa
450 psi
2 in/min; ASTM D638
Elongation at Break 800 %
800 %
2 in/min; ASTM D638