Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data)

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer Quadrant Engineering Plastics Products
Trade Name Symalit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical properties and outstanding chemical and heat resistance Almost unlimited resistance to chemicals Widest service temperature range from - 190 °C up to + 260 °C (- 310 °F up to + 500 °F) Very low permeation values Excellent stress cracking resistance Very low leach-out values for high purity applications Excellent abrasion resistance Excellent ageing stability Resistance to UV-, ß- and gamma -rays High dielectric and piezoelectric values Clear (translucent)
Physical Properties Metric English Comments
Density 2.14 g/cc
0.0773 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 0.010 %
0.010 %
50% RH
Water Absorption at Saturation <= 0.030 %
<= 0.030 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 70
70
ISO 2039-2
Hardness, Shore D 57
57
Ball Indentation Hardness 35.0 MPa
5080 psi
ISO 2039-1
Tensile Strength 15.0 MPa
2180 psi
at Yield; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/-2
Elongation at Yield 50 %
50 %
ISO 527-1/-2
Tensile Modulus 0.575 GPa
83.4 ksi
ISO 527-1/-2
Flexural Strength 18.5 MPa
2680 psi
Compressive Strength 5.50 MPa

@Strain 1 %
798 psi

@Strain 1 %
ISO 604
10.0 MPa

@Strain 2 %
1450 psi

@Strain 2 %
ISO 604
16.0 MPa

@Strain 5 %
2320 psi

@Strain 5 %
ISO 604
K Factor (ISO) 1450 µm/km
1450 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 7.50 J/cm²
35.7 ft-lb/in²
Partial Break; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.25 - 0.35
0.25 - 0.35
Thermal Properties Metric English Comments
CTE, linear 135 µm/m-°C

@Temperature 23.0 - 100 °C
75.0 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
Melting Point 305 °C
581 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 2.1

@Frequency >=100000 Hz
2.1

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
889 kV/in
Dissipation Factor <= 0.00050

@Frequency 100000 Hz
<= 0.00050

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA Yes
Yes
only natural
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Limited
Limited
Continuous Sunlight Limited
Limited
Hot Water / Steam Acceptable
Acceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Unacceptable
Unacceptable