Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.14 g/cc | 0.0773 lb/in³ | ISO 1183-1 |
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data) Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop.. |
|||
Density | 2.14 g/cc | 0.0773 lb/in³ | ASTM D4894 |
3M Dyneon™ CC622 PTFE 10% Graphite Filled
(discontinued **) Product Form: Black, pelletized free-flowing powder. Applications include bearings, ring seals.Data provided by Dyneon. |
|||
Density | 2.14 g/cc | 0.0773 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TF 4212 PTFE 10% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Density | 2.14 g/cc | 0.0773 lb/in³ | Sintered moldings; ASTM D4894/D4895 |
3M Dyneon™ TFM™ 4212 Modified PTFE, 10% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Density | 2.14 - 2.18 g/cc | 0.0773 - 0.0788 lb/in³ | ASTM D792 |
Guarniflon PTFE G400 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Density | 2.14 - 2.19 g/cc | 0.0773 - 0.0791 lb/in³ | ASTM D792 |
Guarniflon PTFE G500 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Density | 2.14 - 2.18 g/cc | 0.0773 - 0.0788 lb/in³ | ASTM D792 |
Guarniflon PTFE G800 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Density | 2.14 - 2.17 g/cc | 0.0773 - 0.0784 lb/in³ | ASTM D792 |
Guarniflon FEP Fluorinated Ethylene Propylene Fluorinated thermoplastic material with excellent thermal, electrical and chemical inertness properties. Widely used for different industrial applications for its excellent chemical resistance up t.. |
|||
Density | 2.14 g/cc | 0.0773 lb/in³ | |
LATI Laticonther 82 CP1/800 PA12 High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Density | 2.14 g/cc | 0.0773 lb/in³ | ASTM D792 |
Ensinger XP-46 Compression Molded Unfilled PCTFE PCTFE is a high performance crystalline polymer with excellent chemical resistance. Because of its low moisture absorption, PCTFE can operate in a continuous service temperature of -250°F to 300°F.. |
|||
Density | 2.14 g/cc | 0.0773 lb/in³ | |
BASF Heligoen® Green L 8730 Color Additive Description: Brilliant phthalocyanine greens, somewhat yellower than L 8690(L 8731 is especially for powder coatings)Chemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable fo.. |
|||
Density | 2.14 g/cc | 0.0773 lb/in³ | |
BASF Heligoen® Green L 8731 Color Additive Description: Brilliant phthalocyanine greens, somewhat yellower than L 8690(L 8731 is especially for powder coatings)Chemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable fo.. |