Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 15.0 MPa | 2180 psi | ASTM D412 |
Multibase TPSiV® 3111-70A Thermoplastic Elastomer TPSiV™ material for injection molding and extrusion applicationsAPPLICATIONS: Solution for appliance, sports and leisure, and construction applications where excellent hydrolysis resistance, high a.. |
|||
Tensile Strength | >= 15.0 MPa | >= 2180 psi | Type IV, 500mm/min; ASTM D638 |
S&E Specialty Polymers XP23-566-1 PVC Description: PVC weatherable, integral colored, filledApplication: Low gloss lift gate molding compound which meets Chrysler MSDC 543.Information provided by S&E Specialty Polymers |
|||
Tensile Strength | >= 15.0 MPa | >= 2180 psi | Type IV, 500mm/min; ISO 37 |
S&E Specialty Polymers XP44-11 PVC Description: PVC weatherable, integral colored, filledApplication: Body side skin extrusion and injection molding compound meets GMP.PVC.015, GMP.PVC.093, GMP.PVC.094, Chrysler MSDC 543, and Ford WS.. |
|||
Tensile Strength | >= 15.0 MPa | >= 2180 psi | DIN 53504 |
NEXA® PFX9014 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
Tensile Strength | 15.0 MPa | 2180 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data) Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop.. |
|||
Tensile Strength | 15.0 MPa | 2180 psi | ASTM D2095 |
Permabond UV649 UV-curable Adhesive PERMABOND UV649 is a single part, fast setting, and UV curable adhesive designed specifically for bonding plastics. This material has excellent adhesion to a variety of plastics including polycarbon.. |
|||
Tensile Strength | >= 15.0 MPa | >= 2180 psi | Type IV, 500mm/min; ISO 37 |
S&E Specialty Polymers XP110-13-45 PVC Description: PVC weatherable, integral colored, filledApplication: Body side end cap extrusion and injection molding compound designed for anti-stain which meets GMP.PVC.093, GMP.PVC.094 & Chrysler .. |
|||
Tensile Strength | 15.0 - 20.0 MPa | 2180 - 2900 psi | ASTM D4894 |
Isoflon PTFE + 50% Stainless Steel (AISI 316 L) Polytetrafluoroethylene with 50% INOX Stainless Steel Properties:Improved compression resistance (very low cold flow)Low permeabilityApplications: Dynamic seals operating under high pressure and when chemical resistance is a necessity.Information prov.. |
|||
Tensile Strength | 15.0 - 20.0 MPa | 2180 - 2900 psi | molded; ASTM D4745 |
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon® |
|||
Tensile Strength | 15.0 - 20.0 MPa | 2180 - 2900 psi | molded; ASTM D4894, ASTM D4745 |
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high .. |
|||
Tensile Strength | 15.0 - 35.0 MPa | 2180 - 5080 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Tensile Strength | 15.0 - 35.0 MPa | 2180 - 5080 psi | Moulding Direction; BS2782:Pt3 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Tensile Strength | 15.0 MPa @Strain 100 % |
2180 psi @Strain 100 % |
ISO 37 |
BASF Elastollan 1198 A TPUR Description: Thermoplastic Polyether Polyurethane Elastomers with outstanding hydrolysis resistance, low temperature flexibility and resistance to micro-organisms.Typical Applications: Cable sheathi.. |
|||
Tensile Strength | 15.0 MPa @Strain 300 % |
2180 psi @Strain 300 % |
ISO 37 |
BASF Elastollan B 85 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | 15.0 MPa | 2180 psi | |
AlphaGary Megolon™ IN200 Low Smoke Halogen Free General purpose insulation grade suitable for use up to 1KV. Application examples include Radio Frequency / Data Optical / Special Fire Survival. |
|||
Tensile Strength | 15.0 MPa | 2180 psi | |
AlphaGary Megolon™ S300 Low Smoke Halogen Free General purpose sheathing compound with good mechanical and processing properties. Application examples include Data, Optical / Radio Frequency. |
|||
Tensile Strength | 15.0 MPa | 2180 psi | fill; ISO 37 Type 2 |
Rogers Corporation Bisco® A2 R 1.5 Engineered Solid Silicone Mass Layer, Fiberglass Reinforced Sound Barrier BISCO® A2 Fiberglass Reinforced Sound Barrier provides a similar level of sound absorption and flame resistance as the non-reinforced A2 Sound Barrier with the addition of increased tensile and tea.. |
|||
Tensile Strength | 15.0 MPa @Strain 20.0 % |
2180 psi @Strain 20.0 % |
ISO 37 |
BASF Elastollan S 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | 15.0 - 20.0 MPa | 2180 - 2900 psi | molded; ASTM D4894, ASTM D4745 |
Guarniflon PTFE G412 Polytetrafluoroethylene 15% Graphite PTFE G Standard Compound with graphite.Properties: Extremely low coefficient of friction. Fairly good compressive strength. Enhanced chemical resistance. Good wear resistance. Good thermal diss.. |
|||
Tensile Strength | >= 15.0 MPa | >= 2180 psi | extruded; ASTM D4894, ASTM D4745 |
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |