Mechanical Properties Metric English Comments
Compressive Strength 10.0 MPa

@Strain 1 %
1450 psi

@Strain 1 %
ISO 604
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data)
FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application..
Compressive Strength 10.0 MPa

@Strain 2 %
1450 psi

@Strain 2 %
ISO 604
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data)
Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop..
Compressive Strength 10.0 MPa

@Strain 2 %
1450 psi

@Strain 2 %
ISO 604
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data)
Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The..
Compressive Strength 10.0 MPa

@Strain 2 %
1450 psi

@Strain 2 %
ISO 604
Quadrant EPP TIVAR® DS PE-UHMW + additives (ISO Data)
TIVAR DS is a modified PE-UHMW with extremely high molecular weight. The latter in combination with a particular manufacturing process result in a PE-UHMW grade with superior wear and abrasion resis..
Compressive Strength 10.0 MPa

@Strain 2 %
1450 psi

@Strain 2 %
ISO 604
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data)
TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low..
Compressive Strength 10.0 MPa

@Temperature 815 °C
1450 psi

@Temperature 1500 °F
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrocast SC-2600 is a high purity silicon carbide based refractory for applications requiring high thermal conductivity, resistance to metal and flame abrasion.ApplicationsFilter boxes Burner tubes ..
Compressive Strength 10.0 - 20.0 MPa

@Temperature 1300 °C
1450 - 2900 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 145 F Sp Dense Refractory Castable
Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variet..
Compressive Strength 10.0 - 20.0 MPa

@Temperature 815 °C
1450 - 2900 psi

@Temperature 1500 °F
Cold Crushing Strength
Gouda Vuurvast CURON 100 Dense Refractory Castable
Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modification..
Copyright © lookpolymers.com All Rights Reserved