Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 2.14 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 2.14 g/cc
0.0773 lb/in³
ISO 1183-1
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data)
Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop..
Density 2.14 g/cc
0.0773 lb/in³
ASTM D4894
3M Dyneon™ CC622 PTFE 10% Graphite Filled  (discontinued **)
Product Form: Black, pelletized free-flowing powder. Applications include bearings, ring seals.Data provided by Dyneon.
Density 2.14 g/cc
0.0773 lb/in³
Sintered moldings; ASTM D4894/D4895
3M Dyneon™ TF 4212 PTFE 10% Electrocarbon Filled  (discontinued **)
Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon.
Density 2.14 g/cc
0.0773 lb/in³
Sintered moldings; ASTM D4894/D4895
3M Dyneon™ TFM™ 4212 Modified PTFE, 10% Electrocarbon Filled  (discontinued **)
Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon.
Density 2.14 - 2.18 g/cc
0.0773 - 0.0788 lb/in³
ASTM D792
Guarniflon PTFE G400 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Density 2.14 - 2.19 g/cc
0.0773 - 0.0791 lb/in³
ASTM D792
Guarniflon PTFE G500 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Density 2.14 - 2.18 g/cc
0.0773 - 0.0788 lb/in³
ASTM D792
Guarniflon PTFE G800 Polytetrafluoroethylene
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif..
Density 2.14 - 2.17 g/cc
0.0773 - 0.0784 lb/in³
ASTM D792
Guarniflon FEP Fluorinated Ethylene Propylene
Fluorinated thermoplastic material with excellent thermal, electrical and chemical inertness properties. Widely used for different industrial applications for its excellent chemical resistance up t..
Density 2.14 g/cc
0.0773 lb/in³
LATI Laticonther 82 CP1/800 PA12
High thermal conductivity product based on Polyamide 12 (PA12). Special fillerAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Density 2.14 g/cc
0.0773 lb/in³
ASTM D792
Ensinger XP-46 Compression Molded Unfilled PCTFE
PCTFE is a high performance crystalline polymer with excellent chemical resistance. Because of its low moisture absorption, PCTFE can operate in a continuous service temperature of -250°F to 300°F..
Density 2.14 g/cc
0.0773 lb/in³
BASF Heligoen® Green L 8730 Color Additive
Description: Brilliant phthalocyanine greens, somewhat yellower than L 8690(L 8731 is especially for powder coatings)Chemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable fo..
Density 2.14 g/cc
0.0773 lb/in³
BASF Heligoen® Green L 8731 Color Additive
Description: Brilliant phthalocyanine greens, somewhat yellower than L 8690(L 8731 is especially for powder coatings)Chemical Structure: Cu-phthalocyanine, chlorinatePhysical form: PowderSuitable fo..
Copyright © lookpolymers.com All Rights Reserved