Polymer Property : CTE, linear = 75.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 135 µm/m-°C

@Temperature 23.0 - 100 °C
75.0 µin/in-°F

@Temperature 73.4 - 212 °F
Quadrant EPP Symalit® 1000 PFA unfilled, lining industries (ISO Data)
Symalit 1000 PFA is made from a fluoropolymer resin that is a copolymer of tetrafluoroethylene and perfluorovinylether. It exhibits good mechanical properties combined with excellent electrical prop..
CTE, linear 135 µm/m-°C

@Temperature -40.0 - 149 °C
75.0 µin/in-°F

@Temperature -40.0 - 300 °F
ASTM E831
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet)
CTE, linear 135 - 135 µm/m-°C

@Temperature 85.0 - 125 °C
75.0 - 75.0 µin/in-°F

@Temperature 185 - 257 °F
Average value: 135 µm/m-°C Grade Count:2
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
CTE, linear 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Spartech Royalite R61M Low Smoke Resin
Data provided by the manufacturer. Formulated to meet smoke and fire specifications recommended by the FTA, this is ideally suited for mass transit applications such as seat backs, overhead storage..
CTE, linear 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Covestro Bayflex® 180 Polyurethane Elastomeric RIM, 20% Mica Filled, MDI-based 2-Component Liquid System
0.150 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and ..
CTE, linear 135 µm/m-°C
75.0 µin/in-°F
ASTM E831
BASF Ultramid® 8270 HS BK 102 PA6 (Dry)
Description: Ultramid 8270 HS BK-102 is a thermally modified pigmented black, PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile ex..
CTE, linear 135 µm/m-°C

@Temperature -30.0 - 30.0 °C
75.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM Test
BASF Ultramid® 8270 HS PA6 (Dry)
Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi..
CTE, linear 135 µm/m-°C

@Temperature 20.0 °C
75.0 µin/in-°F

@Temperature 68.0 °F
Dow Pellethane® 2354-55D Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2354-55D is elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyureth..